References
- Alvino A, Lega D, Giacobbe F, Mazzochi V and Rinaldi A: ‘Damage characterization in two reformer heater tubes after nearly 10 years of service at different operative and maintenance conditions’, Eng. Fail. Ana., 2010, 17, 1526–1541.
- Korkhaus J: ‘Failure mechanisms and material degradation processes at high temperatures in ammonia synthesis’, Corr. Eng. Sci. Technol., 2005, 40, (3), 204–210.
- Khodamorad SH, Haghshenas-Fatmehsari D, Rezaie H and Sadeghipour A: ‘Analysis of ethylene cracking furnace tubes’, Eng. Fail. Ana., 2012, 21, 1–8.
- Ackermann H, Karduck P, Koehne H, Lucks K and von Richthofen A: ‘Metal dusting in low-NOx recirculation burners for fuel oil’, Corros. Eng. Sci. Technol., 2005, 40, (3), 233–238.
- Agüero A, Gutiérrez M, Korcakova L, Nguyen TTM, Hinnemann B and Saadi S: ‘Metal dusting protective coatings A literature review’, Ox. Met., 2011, 76, 23–42.
- Milwar GR, Evans HE, Aindow M and Mowforth CW: ‘The influence of oxide layers on the initiation of carbon deposition on stainless steel’, Ox. Met., 2001, 56, 231–250.
- Wolf I and Grabke HJ: ‘A study on the solubility and distribution of carbon in oxides’, Solid State Commun., 1985, 54, (1), 5–10.
- Rosado C and Schütze M: ‘Protective behavior of newly developed coatings against metal dusting’, Mater. Corros., 2003, 54, (11), 831–853.
- Johnson DF and Carter EA: ‘First principles assessment of carbon absorption into FeAl and Fe3Si: toward prevention of cementite formation and metal dusting of steels’, J. Phys. Chem. C, 2010, 114C, 4436–4444.
- Melo-Máximo L, Salas O, Melo-Máximo D, Oseguera J, López-Hirata VM, Lepienski CM, Torres RD and Souza RM: ‘Performance of Cr oxide coatings on 304 steel against metal dusting’, Surf. Coat. Technol., 2013, 237, 39–50.
- Melo D, Sigüenza D, Salas O, Oseguera J, Reichelt R and López VM: ‘Production, characterization and evaluation of protective Cr oxide coatings against metal dusting’, Surf. Coat. Technol., 2009, 204, (6–7), 788–792.
- Alvarez J, Melo D, Salas O, Reichelt R, Oseguera J and López V: ‘Role of Al oxide PVD coatings in the protection against metal dusting’, Surf. Coat. Technol., 2009, 204, 779–783.
- Sheward JA: ‘The coating of internal surfaces by PVD’, Surf. Coat. Technol., 1992, 54–55, 297–302.
- Chang C.-H and Tsai W.-T: ‘Carburization behavior under pits induced by metal dusting in 304L and 347 stainless steels’, Mater. Chem. Phys., 2009, 116, 426–432.
- Campillo B, González C, Hernández G and Juarez-Islas JA: ‘Temperature corrosion observed in austenitic coils and tubes in a direct reduction process’, J. Mater. Eng. Perfom., 2000, 9, (1), 88–94.
- ‘Standard test method for adhesion strength and mechanical failure modes of ceramic coatings by quantitative single point scratch testing’, C1624-05, ASTM, Philadelphia, PA, USA, 2010.
- Gheno T, Monceau D and Young D: ‘Mechanism of breakaway oxidation of Fe–Cr and Fe–Cr–Ni alloys in dry and wet carbon dioxide’, Corros. Sci., 2012, 64, 222–233.
- Kelly PJ, Hisek J, Zhou Y, Pilkington RD and Arnell RD: ‘Advanced coatings through pulsed magnetron sputtering’, Surf. Eng., 2004, 20, (3), 157–162.
- Lundin D and Sarakinos K: ‘An introduction to thin film processing using high-power impulse magnetron sputtering’, J. Mater. Res., 2012, 27, (5), 780–792.