Publication Cover
Advances in Applied Ceramics
Structural, Functional and Bioceramics
Volume 112, 2013 - Issue 5
80
Views
6
CrossRef citations to date
0
Altmetric
Original Article

Synthesis and characterisation of dental composite materials reinforced with fluoroapatite–mullite glass–ceramic particles

, , , &
Pages 294-300 | Received 14 Nov 2012, Accepted 30 Dec 2012, Published online: 18 Nov 2013

References

  • Shah M, Ferracane J, Kruzic J: ‘R-curve behavior and micromechanisms of fracture in resin based dental restorative composites’, J. Mech. Behav. Biomed., 2009, 2, 502–511.
  • Marchan S, White D, Smith W, Coldero L, Dhuru V: ‘Comparisn of the mechanical properties of two nano filled composite materials’, Rev. Clín. Pesq. Odontol., 2009, 5, 241–246.
  • Johnson W, Dhuru V, Brantley W: ‘Composite microfiller content and its effect on fracture toughness and diametral tensile strength’, Dent. Mater., 1993, 9, 95–98.
  • Brosh T, Ganor Y, Belov I, Pilo R: ‘Analysis of strength properties of light-cured resin composites’, Dent. Mater., 1999, 15, 174–179.
  • Aguiar F, Braceiroa A, Ambrosanob G, Lovadino J: ‘Hardness and diametral tensile strength of a hybrid composite resin polymerized with different modes and immersed in ethanol or distilled water media’, Dent. Mater., 2005, 21, 1098–1103.
  • Xu H, Quinn J, Smith D, Giuseppetti A, Eichmiller F: ‘Effects of different whiskers on the reinforcement of dental resin composites’, Dent. Mater., 2003, 19, 359–367.
  • Guo G, Fan Y, Zhang J, Hagan J, Xu X: ‘Novel dental composites reinforced with zirconia–silica ceramic nanofibers’, Dent. Mater., 2012, 28, 360–368.
  • Xu H, Eichmiller F, Antonucci J, Schumacher G, Ives L: ‘Dental resin composites containing ceramic whiskers and precured glass ionomer particles’, Dent. Mater., 2000, 16, 356–363.
  • Curtis A, Palin W, Fleming G, Shortall A, Marquis M: ‘The mechanical properties of nanofilled resin-based composites: the impact of dry and wet cyclic pre-loading on bi-axial flexure strength’, Dent. Mater., 2009, 25, 188–197.
  • Samuel S, Li S, Mukherjee I, Guo Y, Patel A, Baran G: ‘Mechanical properties of experimental dental composites containing a combination of mesoporous and nonporous spherical silica as fillers’, Dent. Mater., 2009, 25, 296–301.
  • Xu H, Moreau J, Sun L, Chow L: ‘Novel CaF2 Nanocomposite with high strength and fluoride ion release’, J. Dent. Res., 2010, 89, 739–745.
  • Xu H, Moreau J, Sun L, Chow L: ‘Strength and fluoride release characteristics of a calcium fluoride based dental nanocomposite’, Biomaterials, 2008, 29, 4261–4267.
  • Clifford A, Hill R: ‘Apatite–mullite glass–ceramics’, J. Non-Cryst. Solids, 1996, 196, 364–351.
  • Aksay I, Dabbs D, Sarikaya M: ‘Mullite processing, structure, and properties’, J. Am. Ceram. Soc., 1991, 74, 2343–2358.
  • Arcis R, Macipe A, Toledano M, Osorio E, Rodriguez-Clemente R, Murtra J: ‘Mechanical properties of visible Light-cured resins reinforced with hydroxyapatite for dental restoration’, Dent. Mater., 2002, 18, 49–57.
  • Domingo C, Arcıs R, Macip A, Osorio E, Osorio R, Rodriguez-Clemente R: ‘Dental composites reinforced with hydroxyapatite: Mechanical behavior and absorption/elution characteristics’, J. Biomed. Mater. Res., 2001, 56, 297–305.
  • Domingo C, Arcıs R, Osorio E, Osorio R, Fanovich M, Rodríguez-Clemente R: ‘Hydrolytic stability of experimental hydroxyapatite-filled dental composite materials’, Dent. Mater., 2003, 19, 478–486.
  • Montazeri L, Javadpour J, Shokrgozar M, Bonakdar S, Javadian S: ‘Hydrothermal synthesis and characterization of hydroxyapatite and fluorhydroxyapatite nano-size powders’, Biomed. Mater., 2010, 5, 1–7.
  • Mollazadeh S, Eftekhari B, Javadpuor J, Yuosefi A, Jafarzade T: ‘The role of TiO2, ZrO2, BaO and SiO2 on the mechanical properties and crystallization behavior of fluorapatite–mullite glass–ceramics’, J. Non-Cryst. Solids, 2012, to be published.
  • Höland W, Rheinberger V, Apel E, Dommann A, Obrecht M: ‘Clinical applications of glass-ceramics in dentistry’, J. Mater. Sci: Mater. Med., 2006, 17, 1037–1042.
  • Tan Y, Liu Y, Grover L, Huang B: ‘Wear behavior of light-cured dental composites filled with porous glass–ceramic particles’, J. Mech. Behav. Biomed., 2010, 3, 77–84.
  • Liu Y, Tan Y, Lei T, Xiang Q, Han Y, Huang B: ‘Effect of porous glass–ceramic fillers on mechanical properties of light-cured dental resin composites’, Dent. Mater., 2009, 25, 709–715.
  • Xu H: ‘Dental composite resins containing silica-fused ceramic single-crystalline whiskers with various filler levels’, J. Dent. Res., 1999, 78, 1304–1311.
  • Shelby J: ‘Properties of alkali and alkaline earth metaphosphate glasses’, J. Non-Cryst. Solids, 2000, 263, 271–276.
  • Sideridou I, Karabela M: ‘Effect of the amount of 3-methacyloxypropyltrimethoxysilane coupling agent on physical properties of dental resin nanocomposites’, Dent. Mater., 2009, 25, 1315–1324.
  • Hedzelek W, Wachowiak R, Marcinkowsk M, Domka L: ‘Infrared spectroscopic identification of chosen dental materials and natural teeth’, Acta Physica Polonica A, 2008, 114A, 471–484.
  • Beatty M, Swartz M, Moore B, Phillips R, Roberts T: ‘Effect of microfiller fraction and silane treatment on resin composite properties’, J. Biomed. Mater. Res., 1998, 40, 12–23.
  • Halvorson R, Erickson R, Davidson C: ‘The effect of filler and silane content on conversion of resin-based composite’, Dent. Mater., 2003, 19, 327–333.
  • Scougall-Vilchis R, Hotta Y, Hotta M, Idona T, Yamamoto M: ‘Examination of composite resins with electron microscopy, microhardness tester and energy dispersive X-ray microanalyzer’, Dent. Mater., 2009, 28, 102–112.
  • Deb S, Sehm H: ‘A comparative study of the properties of dental resin composites polymerized with plasma and halogen light’, Dent. Mater., 2003, 19, 517–522.
  • Della Bona A, Benetti P, Borba M, Cecchetti B: ‘Flexural and diametral tensile strength of composite resins’, Braz. Oral Res., 2008, 22, 84–89.
  • Walker M, Haj-Ali R, Wang Y, Hunziker D, William K: ‘Influence of environmental conditions on dental composite flexural properties’, Dent. Mater., 2006, 22, 1002–1007.
  • Rodrigues S, Ferracaneb J, Della Bona A: ‘Flexural strength and Weibull analysis of a microhybrid and a nanofill composite evaluated by 3- and 4-point bending tests’, Dent. Mater., 2008, 24, 426–431.
  • Casselli D, Worschech C, Paulillo L, Dias C: ‘Diametral tensile strength of composite resins submitted to different activation techniques’, Braz. Oral Res., 2006, 20, 214–218.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.