Mechanical Properties of Ductile Cast Iron and Cast Steel for Intermediate Level Waste Transport Containers

Pages 193-200 | Published online: 19 Jul 2013

  • IAEA. Regulations for the Safe Transport of Radioactive Materials - 1985 Edition ( As Amended 1990) Safety Series No 6 (Vienna: IAEA) (1990).
  • Smith, M. J. S., Gray, I. L. S., Sievwright, R. W. T., Miles, J. C., Egid, B. and Donelan, P. Investigation into the use of Ductile Cast Iron and Cast Steel for Transport Containers with Plastic Flow Shock Absorbers. In: Proc. PATRAM'92, Yokohama, September 1992, pp. 1113–1120.
  • Metallic Materials-Tensile Testing - Part 1: Method of Test (at ambient temperature). ES EN 10 002 Part 1 (March 1990).
  • Charpy Impact Test on Metallic Materials. BS EN 10 045–1, Part 1 (1990).
  • Fracture Mechanics Toughness Tests. BS 7448; Part 1 ( British Standards Institution) (1991).
  • Standard Test Method for Jic, a Measure of Fracture Toughness, ASTM E813–87.
  • Salzbrenner, R., Sorensen, K. B. and Wellman, G. W. Application of LEFM Design to Nuclear Material Transport Casks. Int. J. Radioact. Mater. Transp. 1(1), 33–40 (1990).
  • British Standard Method for Determination of the Dynamic Fracture Toughness of Metallic Materials. BS 6729 (British Standards Institution) (1987).
  • European Group on Fracture. Project to Develop a Standard method of Fracture Toughness Testing at Very High Loading Rates. DTI Reference RTP2/155/78, 1990. Final report, Appendix 1: Proposed Method for Determination of Dynamic Frac-ture Toughnem of Metallic Materials at Very High Loading Rates (1990).
  • Salzbrenner, R. and Crenshaw, T. Multiple Specimen .1-Integral Testing at Intermediate Rates. J. Exp. Mech., September, p. 217 (1990).
  • Mead, H. and Bradley, W. Fracture Toughness Studies of Ductile Cast Iron Using a J-Integral Approach. Trans. Am. Foundrymen's Soc. p. 265 (1980).
  • Priest, A. Size Effects in Fracture Toughness Testing Procedures. In: Proc. IMechE Seminar on Size Effects in Fracture, RAF Farnborough, 10 Nov. 1986, p. 53.
  • Wallin, K. The Size Effect in K, c Results. Eng. Fract. Mech, 22(1), 149–163 (1985).
  • IAEA. Guidelines for Safe Design of Shipping Packages against Brittle Fracture. TECDOC-717 Vienna: IAEA (1993).
  • Ultrasonic Testing of Ferritic Steel Castings including Quality Levels. BS 6208 (British Standards Institution) (1990).
  • OASYS DYNA3D, Version 5.1 (Oasys Ltd, 13 Fitzroy St., London W1P 6BQ) (September 1992).

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.