Kinetics of In Vitro Lysozyme Deposition on Silicone Hydrogel, PMMA, and FDA Groups I, II, and IV Contact Lens Materials

, , , &
Pages 787-796 | Received 25 May 2005, Accepted 25 Jun 2006, Published online: 02 Jul 2009
 

Abstract

We sought to compare the kinetics of in vitro lysozyme deposition on silicone hydrogel (SH), polymethyl methacrylate (PMMA), and FDA groups I, II, and IV contact lenses. Lenses were incubated in 125I-labeled lysozyme for time periods ranging from 1 hr to 28 days, and radioactive counts were determined. SH lenses and PMMA deposited less lysozyme than conventional hydrogel lenses (p < 0.05). Lysozyme accumulation on group IV lenses reached a maximum on the seventh day and then plateaued, whereas on groups I, II, and SH lenses, deposition continued to increase across all time periods, reiterating that kinetics of lysozyme deposition is highly material dependent.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.