27
Views
23
CrossRef citations to date
0
Altmetric
Original Articles

A Comparison of Fatigue Failure Morphology Between TiN Coated and Uncoated Lubricated Rollers

, , &
Pages 408-416 | Published online: 25 Mar 2008

Keep up to date with the latest research on this topic with citation updates for this article.

Read on this site (2)

J. Neubrand, C. Bilgen & H. Weiss. (1995) Rolling wear of tin coatings induced by non-uniform hertzian stress distribution. Surface Engineering 11:2, pages 133-137.
Read now
L. Chang & W. Zhao. (1995) Wavelength Dependence of Micro-EHL Pressure Rippling with Random Surface-Roughness Profiles. Tribology Transactions 38:2, pages 389-395.
Read now

Articles from other publishers (21)

Yansheng Ma, Jiangfeng Hu & Xuecheng Dong. (2021) A review of physical vapor deposition coatings for rolling bearings. Proceedings of the Institution of Mechanical Engineers, Part J: Journal of Engineering Tribology 236:4, pages 786-803.
Crossref
Bryan Allison. 2021. Failure Analysis and Prevention. Failure Analysis and Prevention 716 729 .
A V Borgaonkar & I Syed. (2020) Effect of coatings on rolling contact fatigue and tribological parameters of rolling/sliding contacts under dry/lubricated conditions: a review. Sādhanā 45:1.
Crossref
Diego Alejandro Colombo, María Dolores Echeverría, Ricardo Cesar Dommarco & Juan Miguel Massone. (2016) Influence of TiN coating thickness on the rolling contact fatigue resistance of austempered ductile iron. Wear 350-351, pages 82-88.
Crossref
Diego Alejandro Colombo, María Dolores Echeverría, Sebastián Laino, Ricardo Cesar Dommarco & Juan Miguel Massone. (2013) Rolling contact fatigue resistance of PVD CrN and TiN coated austempered ductile iron. Wear 308:1-2, pages 35-45.
Crossref
R. Ahmed. 2002. Failure Analysis and Prevention. Failure Analysis and Prevention 941 956 .
I. A. Polonsky & L. M. Keer. (2002) Numerical Analysis of the Effect of Coating Microstructure on Three-Dimensional Crack Propagation in the Coating Under Rolling Contact Fatigue Conditions. Journal of Tribology 124:1, pages 14-19.
Crossref
Jun Qi, C.Y. Chan, I. Bello, C.S. Lee, S.T. Lee, J.B. Luo & S.Z. Wen. (2001) Film thickness effects on mechanical and tribological properties of nitrogenated diamond-like carbon films. Surface and Coatings Technology 145:1-3, pages 38-43.
Crossref
I.A. Polonsky & L.M. Keer. 2001. Tribology Research: From Model Experiment to Industrial Problem - A Century of Efforts in Mechanics, Materials Science and Physico-Chemistry, Proceedings of the 27th Leeds-Lyon Symposium on Tribology. Tribology Research: From Model Experiment to Industrial Problem - A Century of Efforts in Mechanics, Materials Science and Physico-Chemistry, Proceedings of the 27th Leeds-Lyon Symposium on Tribology 799 810 .
C. Sakae & L. M. Keer. (2016) The Effect of a Layer on a 3-D Crack within the Substrate of a Layer/Substrate System. Mathematics and Mechanics of Solids 3:4, pages 433-446.
Crossref
A. Matthews, A. Leyland, K. Holmberg & H. Ronkainen. (1998) Design aspects for advanced tribological surface coatings. Surface and Coatings Technology 100-101, pages 1-6.
Crossref
I.A. Polonsky, T.P. Chang, L.M. Keer & W.D. Sproul. (1998) A study of rolling-contact fatigue of bearing steel coated with physical vapor deposition TiN films: Coating response to cyclic contact stress and physical mechanisms underlying coating effect on the fatigue life. Wear 215:1-2, pages 191-204.
Crossref
I.A. Polonsky, T.P. Chang, L.M. Keer & W.D. Sproul. (1997) An analysis of the effect of hard coatings on near-surface rolling contact fatigue initiation induced by surface roughness. Wear 208:1-2, pages 204-219.
Crossref
C. H. Kuo & L. M. Keer. (1995) Three-Dimensional Analysis of Cracking in a Multilayered Composite. Journal of Applied Mechanics 62:2, pages 273-281.
Crossref
. 1994. Coatings Tribology - Properties, Techniques and Applications in Surface Engineering. Coatings Tribology - Properties, Techniques and Applications in Surface Engineering 409 440 .
Robert Thom, Lewis Moore, William D. Sproul & T. Peter Chang. (1993) Rolling contact fatigue tests of reactively sputtered nitride coatings of Ti, Zr, Hf, Cr, Mo, Ti-Al, Ti-Zr and Ti-Al-V on 440C stainless steel substrates. Surface and Coatings Technology 62:1-3, pages 423-427.
Crossref
William D. Sproul, Michael E. Graham, Ming-Show Wong & Paul J. Rudnik. (1993) Reactive unbalanced magnetron sputtering of the nitrides of Ti, Zr, Hf, Cr, Mo, Ti-Al, Ti-Zr and Ti-Al-V. Surface and Coatings Technology 61:1-3, pages 139-143.
Crossref
O.O. Ajayi, A. Erdemir, G.R. Fenske, F.A. Nichols, W.D. Sproul, M. Graham & P.J. Rudnik. (1992) Tribological behavior of oil-lubricated TiN-coated steel. Surface and Coatings Technology 54-55, pages 496-501.
Crossref
Ali Erdemir. (1992) Rolling-contact fatigue and wear resistance of hard coatings on bearing-steel substrates. Surface and Coatings Technology 54-55, pages 482-489.
Crossref
O.O. Ajayi, A. Erdemir, G.R. Fenske, F.A. Nichols, W.D. Sproul, M. Graham & P.J. Rudnik. 1992. Metallurgical Coatings and Thin Films 1992. Metallurgical Coatings and Thin Films 1992 496 501 .
Ali Erdemir. 1992. Metallurgical Coatings and Thin Films 1992. Metallurgical Coatings and Thin Films 1992 482 489 .

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.