Characterizing particle emissions from a direct energy deposition additive manufacturing process and associated occupational exposure to airborne particles

ORCID Icon, , &
Pages 59-72 | Published online: 12 Dec 2019
 

Abstract

This study aims to characterize airborne particles emitted from a metal additive manufacturing machine and related levels of occupational exposure. To achieve this, a complete measurement methodology was deployed around a direct energy deposition machine. Different operating conditions were investigated, based on configurations of two materials and two injection nozzles. Two replicates were performed for each condition. Airborne particles emitted during repeated manufacturing cycles were measured simultaneously at the source, in the near field, in the far field and on the operator. Real-time instruments were used to characterize the machine emissions (10 nm–10 µm) associated with respirable and inhalable samplers and cascade impactors. Measurements were made during both the manufacturing process and transient operating phases. In parallel, personal exposure to hexavalent chromium was assessed. The number of particles measured for the different machining phases show that high levels of particles (> 5 × 105 # cm−3, 0.3–1.3 mg m−3 inhalable particles, 0.2–6 µg m−3 CrVI) were emitted in the machine enclosure. The size distributions indicate that more than 90% of the particles are smaller than 250 nm. Occupational exposure to CrVI was found to be below the LOQ of 0.098 µg m−3 for the two alloys investigated. During the machining process, near-field number and mass concentrations were ∼ 104 # cm−3, and below 0.04 mg m−3, respectively. Far-field number concentrations were also on the order of 104 # cm−3 throughout the whole monitoring period. The transient phase of door opening was found to result in high levels of exposure (> 105 # cm−3), which were also detected in the near-field, confirming the need to implement preventative actions. To address this issue, a collective protective measure, consisting of setting a time delay of about 8 min between the end of the manufacturing process and opening of the door, could be employed. This collective measure should also be accompanied by the wearing of personal protective equipment by the operator when an intervention in the machine enclosure is necessary.

Acknowledgments

The authors would like to thank Mr. Boisselier and Mr. Wursthorn of Irépa Laser for their support and the provision of their additive manufacturing machine. DR would like to acknowledge O. Rastoix, N. Carabin, and H. Poirot from INRS for off-line sample analyses.

Log in via your institution

Log in to Taylor & Francis Online

PDF download + Online access

  • 48 hours access to article PDF & online version
  • Article PDF can be downloaded
  • Article PDF can be printed
USD 61.00 Add to cart

Issue Purchase

  • 30 days online access to complete issue
  • Article PDFs can be downloaded
  • Article PDFs can be printed
USD 148.00 Add to cart

* Local tax will be added as applicable

Related Research

People also read lists articles that other readers of this article have read.

Recommended articles lists articles that we recommend and is powered by our AI driven recommendation engine.

Cited by lists all citing articles based on Crossref citations.
Articles with the Crossref icon will open in a new tab.