898
Views
0
CrossRef citations to date
0
Altmetric
Articles

Investigation of hot workability behavior of as-cast Mg–5Sn–2Ca (TX52) magnesium alloy through processing map

, , , &
Pages 241-252 | Received 19 Nov 2013, Accepted 12 Mar 2014, Published online: 29 Apr 2014

Figures & data

Figure 1. Microstructure of Mg–5Sn–2Ca alloy: (a) optical and (b) SEM images.

Figure 1. Microstructure of Mg–5Sn–2Ca alloy: (a) optical and (b) SEM images.

Figure 2. True stress–true strain curves of Mg–5Sn–2Ca alloy at different strain rates at (a) 350 °C and (b) 550 °C.

Figure 2. True stress–true strain curves of Mg–5Sn–2Ca alloy at different strain rates at (a) 350 °C and (b) 550 °C.

Figure 3. Processing map of Mg–5Sn–2Ca at a strain of .5. The numbers against the contours indicate efficiency of power dissipation in percent and the dark line separates the stable and unstable regions.

Figure 3. Processing map of Mg–5Sn–2Ca at a strain of .5. The numbers against the contours indicate efficiency of power dissipation in percent and the dark line separates the stable and unstable regions.

Figure 4. Microstructure of Mg–5Sn–2Ca deformed at (a) 350 °C/.0003 s−1 (Domain 1) and (b) 550 °C/10 s−1 (Domain 2). The compression axis is vertical.

Figure 4. Microstructure of Mg–5Sn–2Ca deformed at (a) 350 °C/.0003 s−1 (Domain 1) and (b) 550 °C/10 s−1 (Domain 2). The compression axis is vertical.

Figure 5. Microstructure of Mg–5Sn–2Ca specimen deformed in the flow instability regimes at (a) 300 °C/10 s−1 and (b) 300 °C/.1 s−1, exhibiting shear band and flow localization (shown by arrows).

Figure 5. Microstructure of Mg–5Sn–2Ca specimen deformed in the flow instability regimes at (a) 300 °C/10 s−1 and (b) 300 °C/.1 s−1, exhibiting shear band and flow localization (shown by arrows).

Figure 6. Variation of flow stress with strain rate of Mg–5Sn–2Ca alloy at different test temperatures.

Figure 6. Variation of flow stress with strain rate of Mg–5Sn–2Ca alloy at different test temperatures.

Figure 7. Arrhenius plot for calculating apparent activation energy of Mg–5Sn–2Ca alloy at different strain rates.

Figure 7. Arrhenius plot for calculating apparent activation energy of Mg–5Sn–2Ca alloy at different strain rates.