Influence of silicoating, etching and heated glaze treatment on the surface of Y-TZP and its impact on bonding with veneering ceramic

, , , , &
Pages 1055-1065 | Received 04 Apr 2017, Accepted 05 Nov 2017, Published online: 17 Nov 2017

References

  • Albashaireh ZS, Ghazal M, Kern M. Two-body wear of different ceramic materials opposed to zirconia ceramic. J Prosthet Dent. 2010;104:105–113.10.1016/S0022-3913(10)60102-3
  • Raigrodski AJ, Hillstead MB, Meng GK, et al. Survival and complications of zirconia-based fixed dental prostheses: a systematic review. J Prosthet Dent. 2012;107:170–177.10.1016/S0022-3913(12)60051-1
  • Piconi C, Maccauro G. Zirconia as a ceramic biomaterial. Biomaterials. 1999;20:1–25.10.1016/S0142-9612(98)00010-6
  • Manicone PF, Rossi Iommetti P, Raffaelli L. An overview of zirconia ceramics: basic properties and clinical applications. J Dent. 2007;35:819–826.10.1016/j.jdent.2007.07.008
  • Spear F, Holloway J. Which all-ceramic system is optimal for anterior esthetics? J Am Dent Assoc. 2008;139(Suppl):S19–S24.10.14219/jada.archive.2008.0358
  • Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II: zirconia veneering ceramics. Dent Mater. 2006;22:857–863.10.1016/j.dental.2005.11.014
  • Sailer I, Feher A, Filser F, et al. Prospective clinical study of zirconia posterior fixed partial dentures: 3-year follow-up. Quintessence Int. 2006;37:685–693.
  • Sailer I, Feher A, Filser F, et al. Five-year clinical results of zirconia frameworks for posterior fixed partial dentures. Int J Prosthodont. 2007;20:383–388.
  • Schwarz S, Schröder C, Hassel A, et al. Survival and chipping of zirconia-based and metal-ceramic implant-supported single crowns. Clin Implant Dent Relat Res. 2012;14(Suppl 1):e119–e125.10.1111/j.1708-8208.2011.00388.x
  • Larsson C, Vult von Steyern P, Nilner K A prospective study of implant-supported full-arch yttria-stabilized tetragonal zirconia polycrystal mandibular fixed dental prostheses: three-year results. Int J Prosthodont. 2010;23:364–369.
  • Schmitter M, Mussotter K, Rammelsberg P, et al. Clinical performance of long-span zirconia frameworks for fixed dental prostheses: 5-year results. J Oral Rehabil. 2012;39:552–557.10.1111/jor.2012.39.issue-7
  • Pihlaja J, Näpänkangas R, Raustia A. Early complications and short-term failures of zirconia single crowns and partial fixed dental prostheses. J Prosthet Dent. 2014;112:778–783.10.1016/j.prosdent.2014.03.008
  • Donovan TE. Factors essential for successful all-ceramic restorations. J Am Dent Assoc. 2008;139(Suppl):S14–S18.10.14219/jada.archive.2008.0360
  • Guess PC, Kuliš A, Witkowski S, et al. Shear bond strengths between different zirconia cores and veneering ceramics and their susceptibility to thermocycling. Dent Mater. 2008;24:1556–1567.10.1016/j.dental.2008.03.028
  • Ozkurt Z, Kazazoglu E, Unal A. In vitro evaluation of shear bond strength of veneering ceramics to zirconia. Dent Mater J. 2010;29:138–146.10.4012/dmj.2009-065
  • Tada K, Sato T, Yoshinari M. Influence of surface treatment on bond strength of veneering ceramics fused to zirconia. Dent Mater J. 2012;31:287–296.10.4012/dmj.2011-163
  • Pereira G, Venturini A, Silvestri T, et al. Low-temperature degradation of Y-TZP ceramics: a systematic review and meta-analysis. J Mech Behav Biomed Mater. 2016;55:151–163.10.1016/j.jmbbm.2015.10.017
  • Kirmali O, Kapdan A, Kustarci A, et al. Veneer ceramic to Y-TZP bonding: comparison of different surface treatments. J Prosthodont. 2016;25:324–329.10.1111/jopr.2016.25.issue-4
  • Casucci A, Mazzitelli C, Monticelli F, et al. Morphological analysis of three zirconium oxide ceramics: effect of surface treatments. Dent Mater. 2010;26:751–760.10.1016/j.dental.2010.03.020
  • Teng J, Wang H, Liao Y, et al. Evaluation of a conditioning method to improve core-veneer bond strength of zirconia restorations. J Prosthet Dent. 2012;107:380–387.10.1016/S0022-3913(12)60095-X
  • Chaiyabutr Y, McGowan S, Phillips KM, et al. The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic. J Prosthet Dent. 2008;100:194–202.10.1016/S0022-3913(08)60178-X
  • Casucci A, Osorio E, Osorio R, et al. Influence of different surface treatments on surface zirconia frameworks. J Dent. 2009;37:891–897.10.1016/j.jdent.2009.06.013
  • Guazzato M, Quach L, Albakry M, et al. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent. 2005;33:9–18.10.1016/j.jdent.2004.07.001
  • Fischer J, Grohmann P, Stawarczyk B. Effect of zirconia surface treatments on the shear strength of zirconia/veneering ceramic composites. Dent Mater J. 2008;27:448–454.10.4012/dmj.27.448
  • Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Selective infiltration-etching technique for a strong and durable bond of resin cements to zirconia-based materials. J Prosthet Dent. 2007;98:379–388.10.1016/S0022-3913(07)60123-1
  • Aboushelib MN, Matinlinna JP, Salameh Z, et al. Innovations in bonding to zirconia-based materials: Part I. Dent Mater. 2008;24:1268–1272.10.1016/j.dental.2008.02.010
  • Lundberg K, Wu L, Papia E. The effect of grinding and/or airborne-particle abrasion on the bond strength between zirconia and veneering porcelain: a systematic review. Acta Biomater Odontol Scand. 2017;3:8–20.10.1080/23337931.2017.1293486
  • Oñzcan M, Bernasconi M. Adhesion to zirconia used for dental restorations: a systematic review and meta-analysis. J Adhes Dent. 2015;17:7–26.
  • Yamaguchi H, Ino S, Hamano N, et al. Examination of bond strength and mechanical properties of Y-TZP zirconia ceramics with different surface modifications. Dent Mater J. 2012;31:472–480.10.4012/dmj.2011-237
  • Casucci A, Mazzitelli C, Monticelli F, et al. Morphological analysis of three zirconium oxide ceramics: Effect of surface treatments. Dent Mater. 2010;26:751–760.10.1016/j.dental.2010.03.020
  • Lv P, Yang X, Jiang T. Influence of hot-etching surface treatment on zirconia/resin shear bond strength. Materials. 2015;8:8087–8096.10.3390/ma8125409
  • Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Effect of zirconia type on its bond strength with different veneer ceramics. J Prosthodont. 2008;17:401–408.10.1111/jopr.2008.17.issue-5
  • Al-Dohan HM, Yaman P, Dennison JB, et al. Shear strength of core-veneer interface in bi-layered ceramics. J Prosthet Dent. 2004;91:349–355.10.1016/j.prosdent.2004.02.009
  • Kosmač T, Oblak C, Jevnikar P, et al. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic. Dent Mater. 1999;15:426–433.10.1016/S0109-5641(99)00070-6
  • Kosmač T, Oblak C, Jevnikar P, et al. Strength and reliability of surface treated Y-TZP dental ceramics. J Biomed Mater Res. 2000;53:304–313.10.1002/(ISSN)1097-4636

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.