TiB2 embedded borosilicate coatings with improved wear resistance

ORCID Icon, ORCID Icon, ORCID Icon, ORCID Icon & ORCID Icon
Pages 1449-1456 | Received 02 Jul 2021, Accepted 25 Oct 2021, Published online: 11 Nov 2021

References

  • Andrews AI, Pagliuca S, Faust WD. Porcelain (vitreous) enamels – industrial enamelling processes. Mantova: International Enamellers Institute; 2011.
  • Höland W, Beall GH. Glass-ceramic technology. 3rd ed. Hoboken (NJ): JohnWiley & Sons, Inc; 2020.
  • Deubener J, Allix M, Davis MJ, et al. Updated definition of glass-ceramics. J Non Cryst Solids. 2018;501:3–10.
  • McMillan PW. Glass-Ceramics. 2nd ed. London: Academic Press; 1979.
  • Russo F, Rossi S, Compagnoni AM. Porcelain enamel coatings. Encyclopedia. 2021;1(2):388–400.
  • Millar N, Wilson C. Vitreous enamel coatings. In: Shreir LL, Jarman RA, Burstein GT, editors. Corrosion. Oxford: Butterworth-Heinemann; 1994. p. 3–12.
  • Rossi S, Calovi M, Velez D, et al. Influence of addition of hard particles on the mechanical and chemical behaviour of vitreous enamel. Surf Coat Technol. 2019;357:69–77.
  • Rossi S, Russo F, Calovi M. Durability of vitreous enamel coatings and their resistance to abrasion, chemicals, and corrosion: a review. J Coat Technol Res. 2021;18:39–52.
  • Rossi S, Fedel M, Deflorian F, et al. Abrasion and chemical resistance of composite vitreous enamel coatings with hard particles. Surf Interface Anal. 2015;48(8):827–837.
  • Rossi S, Parziani N, Zanella C. Abrasion resistance of vitreous enamel coatings in function of frit composition and particles presence. Wear. 2015;332–333:702–709.
  • Conde A, Damborenea JJ, Degradation of vitreous enamel coatings. In: Cottis B, Graham M, Lindsay R, editors. Shreir's corrosion. Amsterdam: Elsevier Academic Press; 2016. p. 2330–2336.
  • Paran ND, Chen WW. Crack propagation through interfaces in a borosilicate glass and a glass ceramic. Int J Appl Glass Sci. 2014;5(4):353–362.
  • Danzer R, Lube T, Supancic P, et al. Fracture of ceramics. Adv Eng Mater. 2008;10(4):275–298.
  • Hvizdoš P. Wear and erosion resistant ceramic materials. In: Pomeroy M, editor. Encyclopedia of materials: technical ceramics and glasses. Amsterdam: Elsevier; 2021. p. 416–424.
  • Rossi S, Zanella C, Sommerhuber R. Influence of mill additives on vitreous enamel properties. Mater Design. 2014;55:880–887.
  • Chakraborty S, Debnath D, Mallick AR, et al. Mechanical and thermal properties of hot pressed ZrB2 system with TiB2. Int J Refract Met Hard Mater Int. 2014;46:35–42.
  • Shackelford JF, Han Y, Kim S, et al. CRC materials science and engineering handbook. 4th ed. Boca Raton (FL): CRC Press; 2015.
  • Lee DB, Kim MH, Yang CW, et al. The oxidation of TiB2 particle-reinforced TiAl intermetallic composites. Oxid Met. 2001;56(3/4):2001.
  • Adachi K, Kato K. Formation of smooth wear surfaces on alumina ceramics by embedding and tribo-sintering of fine wear particles. Wear. 2000;245(1–2):84–91.
  • Rossi S, Scrinzi E. Evaluation of abrasion resistance of enamel coatings. Chem Eng Process. 2013;68:74–80.
  • TaberIndustries.com [Internet]. New York (NY): Taber Industries; [cited 2021 July 1]. Available from: https://www.taberindustries.com/content/documents/Important%20Notice%20-%20S33%20Sandpaper%20Strips%20%28May%202018%29.pdf/.
  • Bieleman J, Heilen W, Silber S, et al. Surface-active agents. In: Bieleman J, editor. Additives for coatings. Baden-Württemberg: JohnWiley & Sons, Inc; 2000. p. 65–137.
  • Pittoni PG, Chang Y, Lin S. Interpretation of the peculiar temperature dependence of surface tension for boron trioxide. J Taiwan Inst Chem Eng. 2012;43(6):852–859.
  • Brook R. Materials science and technology: processing of ceramics v. 17B: a comprehensive treatment. Weinheim: Wiley; 1996.
  • Nisbet WJ, Lorimer GW, Sherhod C, et al. Dual phase vitreous enamels part 3 transmission electron microscopy of enamel/ substrate interface. Mater Sci Technol. 1990;6(2):182–186.
  • Samiee L, Sarpoolaky H, Mirhabibi A. Influence of bubble structure on adherence and chemical durability of porcelain enamel. Adv Appl Ceram. 2008;107:27–33.
  • King BW, Tripp HP, Duckworth WH. Nature of adherence of porcelain enamels to metals. J Am Ceram Soc. 1959;42(11):504–525.
  • Protasova LG, Kosenko VG, Farafontova EP. Corrosion of steel under enamel coating. Glass Ceram. 2003;60(7–8):229–230.
  • Greenhut VA, Haber RA. Ceramics, ceramic-metal systems. In: Wiley- VCH, editor. Ullmann's encyclopedia of industrial chemistry. Baden-Württemberg: JohnWiley & Sons, Inc.; 2000. p. 551–575.
  • Ibrahhim S, Gomaa MM, Darwish H. Influence of Fe2O3 on the physical, structural and electrical properties of sodium lead borate glasses. J Adv Ceram. 2014;3(2):155–164.
  • Zhong J, Xue J, Huang Y. Effects of Fe2O3 on crystallisation and properties of R2O–CaO–MgO–Al2O3–SiO2–Fe2O3 glass ceramics. Adv Appl Ceram. 2021;120(3):164–168.
  • Rampf M, Fisch M, Helsch G, et al. Quartz-containing glass-ceramics in the SiO2–Li2O–K2O–MgO-CaO–Al2O3–P2O5 system. Appl. Glass Sci. 2018;10(3):1–9.
  • Salman SM, Salama SN, Abo-Mosallam HA. The crystallization behaviour and bioactivity of wollastonite glass-ceramic based on Na2O–K2O–CaO–SiO2–F glass system. J Asian Ceram Soc. 2015;3(3):255–261.
  • Gupta SK, Rajakumar V, Grieveson P. Phase transformations during heating of llmenite concentrates. Metall Trans B. 1991;22:711–716.
  • Santos RLP, Buciumeanu M, Silva FS, et al. Tribological behaviour of glass-ceramics reinforced by Yttria stabilized zirconia. Tribol Int. 2016;102:361–370.
  • Gungor F, Altun B. Development of scratch resistance of soft porcelain opaque glazes. Trans Indian Ceram Soc. 2018;77(4):192–197.
  • Sánchez E, Ibáñez MJ, García-Ten J, et al. Porcelain tile microstructure: implications for polished tile properties. J Eur Ceram Soc. 2006;26(13):2533–2540.
  • Xiao Z, Tan F, Wang W, et al. Oxidation behaviour of glass–quartz and glass–quartz–aluminium composite coatings on Ti–6Al–4V alloy. Surf. Eng. 2015;31(5):361–367.
  • Eilaghi M, Montazerian M, Yekta BE. Effect of partial substitution of K2O for Na2O on sintering, crystallization and mechanical properties of SiO2-CaO-K2O-Na2O-CaF2 glass-ceramics. Trans Indian Ceram Soc. 2016;75(1):1–6.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.