References
- Tanaka, T., “Research on the hydraulic properties of granulated blast furnace slag II”, Rock products, 59 (7), 106, 108, 110 (1956).
- Keil, F. and Locher, F. W., “Hydraulische Eigenschaften von Glasern, I. Glaser des system CaO-SiO2-Al2O3. Ohne und mit MgO”, Zemenl-Kalk-Gips, 11, 245–53 (1958).
- Samaddar, B. N. and Lahiri, D., “Some investigations on the activation of slags of CaO-Al2O3-SiO2system by DTA”, Trans. Ind. Ceram. Soc., 21 (3), 75–85 (1962).
- Parker, T. W., “Influence of heat treatment of Portland Cement Clinker on the properties of Cement”, Jour. Soc. Chem. Ind., 58, 203 (1939).
- Chatterjee, M. K. and Lahiri, D., “Estimation of free Calcium hydroxide present in hydrated cements by differential thermogravimetric analysis”, Trans. Ind. Ceram. Soc. 23 (4), 198–202 (1964).