Preparation and characterisation of silicone-based coatings filled with carbon nanotubes and natural sepiolite and their application as marine fouling-release coatings

, , , , , , , & show all
Pages 291-302 | Received 26 Feb 2008, Accepted 24 Apr 2008, Published online: 06 Oct 2011

References

  • Alexandre , M and Dubois , P . 2000 . Polymer-layered silicate nanocomposites: preparation, properties and uses of a new class of materials . Mater Sci Eng. , R28 : 1 – 63 .
  • Beigbeder , A , Linares , M , Devalkenaere , M , Degée , P , Claes , M , Beljonne , D , Lazzaroni , R and Dubois , P . 2008 . CH-pi interactions as the driving force for silicone-based nanocomposites with exceptional properties . Adv Mater , 20 : 1003 – 1007 .
  • Berglin , M , Lönn , N and Gatenholm , P . 2003 . Coating modulus and barnacle bioadhesion . Biofouling , 19 ( Suppl ) : 63 – 69 .
  • Berntsson , K M , Jonsson , P R , Lejhall , M and Gatenholm , P . 2000 . Analysis of behavioural rejection of micro-textured surfaces and implications for recruitment by the barnacle Balanus improvisus . J Exp Mar Biol Ecol. , 251 : 59 – 83 .
  • Berntsson , K M , Jonsson , P R , Larsson , A I and Holdt , S . 2004 . Rejection of unsuitable substrata as a potential driver of aggregated settlement in the barnacle Balanus improvisus . Mar Ecol Prog Ser. , 275 : 199 – 210 .
  • Beyer , G . 2002 . Nanocomposites: a new class of flame retardants for polymers . Plast Addit Compd. , 4 : 22 – 28 .
  • Bokobza , L . 2004 . Elastomeric composites. I. Silicone composites . J Appl Polym Sci. , 93 : 2095 – 2104 .
  • Bokobza , L and Kolodziej , M . 2006 . On the use of carbon nanotubes as reinforcing fillers for elastomeric materials . Polym Int. , 55 : 1090 – 1098 .
  • Bultman , J D and Griffith , J R . 1994 . “ Fluoropolymer and silicone fouling-release coatings ” . In Recent developments in biofouling control , Edited by: Thompson , M F , Nagabhushanam , R , Sarojini , R and Fingerman , M . 383 Rotterdam : A.A. Balkema .
  • Brady , R F and Singer , I L . 2000 . Mechanical factors favoring release from fouling release coatings . Biofouling , 15 : 73 – 81 .
  • Callow , J A and Callow , M E . 2006 . “ The Ulva spore adhesive system ” . In Biological adhesives Edited by: Smith , A M and Callow , J A . 63 – 78 . Springer-Verlag, Berlin, Heidelberg
  • Callow , M E , Callow , J A , Pickett-Heaps , J D and Wetherbee , R . 1997 . Primary adhesion of Enteromorpha (Chlorophyta, Ulvales) propagules: quantitative settlement studies and video microscopy . J Phycol. , 33 : 938 – 947 .
  • Callow , M E , Callow , J A , Ista , L K , Coleman , S E , Nolasco , A C and Lopez , G P . 2000 . Use of self-assembled monolayers of different wettabilities to study surface selection and primary adhesion processes of green algal (Enteromorpha) zoospores . Appl Environ Microbiol. , 66 : 3249 – 3254 .
  • Callow , M E , Jennings , A R , Brennan , A B , Seegert , C E , Gibson , A , Wilson , L , Feinberg , A , Baney , R and Callow , J A . 2002 . Microtopographic cues for settlement of zoospores of the green fouling alga Enteromorpha . Biofouling , 18 : 237 – 245 .
  • Carman , M L , Estes , T G , Feinberg , A W , Schumacher , J F , Wilkerson , W , Wilson , L H , Callow , M E , Callow , J A and Brennan , A B . 2006 . Engineered antifouling microtopographies––correlating wettability with cell attachment . Biofouling , 22 : 11 – 21 .
  • Cassé , F , Ribeiro , E , Ekin , A , Webster , D C , Callow , J A and Callow , M E . 2007a . Laboratory screening of coating libraries for algal adhesion . Biofouling , 23 : 267 – 276 .
  • Cassé , F , Stafslien , S J , Bahr , J A , Daniels , J , Finlay , J A , Callow , J A and Callow , M E . 2007b . Combinatorial materials research applied to the development of new surface coatings. V. Application of a spinning water-jet for the semi-high throughput assessment of the attachment strength of marine fouling algae . Biofouling , 23 : 121 – 130 .
  • Chaudhury , M K , Finlay , J A , Chung , J Y , Callow , M E and Callow , J A . 2005 . The influence of elastic modulus and thickness on the soft fouling alga Ulva linza (Enteromorpha linza) from polydimethyl siloxane (PDMS) ideal networks . Biofouling , 21 : 41 – 48 .
  • Chaterjee , S , Goyal , A and Shah , S I . 2006 . Inorganic nanocomposites for the next generation photovoltaics . Matter Lett. , 60 : 3541 – 3543 .
  • Chen , C , Wang , J and Chen , Z . 2004 . Surface restructuring behavior of various types of poly(dimethylsiloxane) in water detected by SFG . Langmuir. , 20 : 10186 – 10193 .
  • Chen , H , Zheng , M , Sun , H and Jia , Q . 2007 . Characterization and properties of sepiolite/polyurethane nanocomposites . Mater Sci Eng A. , 445 : 725 – 730 .
  • Clare , A S . 1996 . Marine natural product antifoulants: status and potential . Biofouling , 9 : 211 – 229 .
  • Clare , A S and Matsumura , K . 2000 . Nature and perception of barnacle settlement pheromones . Biofouling , 15 : 57 – 71 .
  • Clare , A S and Høeg , J T . 2008 . Balanus amphitrite or Amphibalanus amphitrite? A note on barnacle nomenclature . Biofouling , 24 : 55 – 57 .
  • Crisp , D J . 1974 . “ Factors influencing the settlement of marine invertebrate larvae ” . In Chemoreception in marine organisms , Edited by: Grant , P T and Mackie , A M . 177 – 265 . London : Academic Press .
  • Crisp , D J and Barnes , H . 1954 . The orientation and distribution of barnacles at settlement with particular reference to surface contour . J Anim Ecol. , 23 : 143 – 162 .
  • Curtis , A SG , Casey , B , Gallagher , J O , Pasqui , D , Wood , M A and Wilkinson , C DW . 2001 . Substratum topography and the adhesion of biological cells. Are symmetry or regularity of nanotopography important? . Biophys Chem. , 94 : 275 – 283 .
  • Dahlström Jonsson , H , Jonsson , P R and Elwing , H . 2004 . Suface wettability as a determinant in the settlement of the barnacle Balanus improvisus (Darwin) . J Exp Mar Biol Ecol. , 305 : 223 – 232 .
  • de Paiva , L B , Morales , A R and Guimaroes , T R . 2007 . Structural and optical properties of polypropylene-montmorillonite nanocomposites . Mater Sci Eng A. , 447 : 261 – 265 .
  • Erva , S , Bahar , I and Erman , B . 1998 . Swelling of sodium chloride filled polybutadiene networks in water, water/acetone and water/THF mixtures . Polymer , 39 : 2035 – 2041 .
  • Finlay , J A , Fletcher , B R , Callow , M E and Callow , J A . 2008 . Effect of background colour on growth and adhesion strength of Ulva sporelings . Biofouling , 24 : 219 – 225 .
  • Fusetani , N . 2004 . Natural products and antifouling . Nat Prod Rep. , 21 : 94 – 104 .
  • Genzer , J and Efimenko , K . 2006 . Review: recent developments in superhydrophobic surfaces and their relevance to marine fouling . Biofouling , 22 : 339 – 360 .
  • Hellio , C , Marechal , J P , Veron , B , Bremer , G , Clare , A S and Le Gal , Y . 2004 . Seasonal variation of antifouling activities of marine algae from the Brittany coast (France) . Mar Biotechnol. , 6 : 67 – 82 .
  • Hellio , C , Tsoukatou , M , Marechal , J P , Aldred , N , Beaupoil , C , Clare , A S , Vagias , C and Roussis , V . 2005 . Inhibitory effects of Meditteranean sponge extracts and metabolites on larval settlement of the barnacle Balanus amphitrite . Mar Biotechnol. , 7 : 297 – 305 .
  • Iijima , S . 1991 . Helical microtubules of graphitic carbon . Nature , 354 : 56 – 58 .
  • Jeffrey , S W and Humphrey , G F . 1975 . New spectrophotometric equations for determining chlorophylls a, b, c1 and c2 in higher plants, algae and natural phytoplankton . Biochem Physiol Pflanz. , 167 : 191 – 194 .
  • Jelic-Mrcelic , G , Sliskovic , M and Antolic , B . 2006 . Biofouling communities on test panels coated with TBT and TBT-free copper-based antifouling paints . Biofouling , 22 : 293 – 302 .
  • Jin , M H , Feng , X J , Xi , J M , Ehai , J , Cho , K W and Feng , L . 2005 . Super-hydrophobic PDMS surfaces with ultra-low adhesive force . Macromol Rapid Commun. , 26 : 1805 – 1809 .
  • Kavanagh , C J , Quinn , R D and Swain , G W . 2005 . Observations of barnacle detachment from silicones using high-speed video . J Adhesion. , 81 : 843 – 868 .
  • Khorazani , M T , Mirzadeh , H and Kermani , Z . 2005 . Wettability of porous polydimethylsiloxane surface: morphology study . Appl Surf Sci. , 242 : 339 – 345 .
  • Kim , J , Chisholm , B J and Bahr , J . 2007 . Adhesion study of silicone coatings: the interaction of thickness, modulus, and shear rate on adhesion force . Biofouling , 23 : 113 – 120 .
  • Lemire , M and Bourget , E . 1996 . Substratum heterogeneity and complexity influence micro-habitat selection of Balanus sp. and Tubulariacrocea larvae . Mar Ecol Prog Ser. , 135 : 77 – 87 .
  • Ma , J , Bilotti , E , Peijs , T and Darr , J A . 2007 . Preparation of polypropylene/sepiolite nanocomposites using supercritical CO2 assisted mixing . Eur Pol J. , 43 : 4931 – 4939 .
  • Marmur , A . 2006 . Superhydrophobicity fundamentals: implications for biofouling prevention . Biofouling , 22 : 107 – 115 .
  • Newby , B M and Chaudhury , M K . 1997 . Effect of interfacial slippage on viscoelastic adhesion . Langmuir. , 13 : 1805 – 1809 .
  • O'Connor , N J and Richardson , D L . 1994 . Comparative attachment of barnacle cyprids (Balanus amphitrite Darwin, 1854; B. improvisus Darwin, 1854; and B. eburneus Gould, 1841) to polystyrene and glass substrata . J Exp Mar Biol Ecol. , 183 : 213 – 225 .
  • Olsen , S M , Pedersen , L T , Laursen , M H , Kiil , S and Dam-Johansen , K . 2007 . Enzyme-based antifouling coatings: a review . Biofouling , 23 : 369 – 383 .
  • Patwardhan , S V , Taori , V P , Hassan , M , Agashe , N R , Franklin , J E , Beaucage , G , Mark , J E and Clarson , S J . 2006 . An investigation of the properties of poly(dimethylsiloxane)-bioinspired silica hybrids . Eur Pol J. , 42 : 167 – 178 .
  • Phang , Y , Aldred , N , Clare , A S , Callow , J A and Vansco , G J . 2006 . An in situ study of the nanomechanical properties of barnacle (Balanus amphitrite) cyprid cement using atomic force microscopy (AFM) . Biofouling , 22 : 245 – 250 .
  • Ramsay , D B , Dickinson , G H , Orihuela , B , Rittschof , D and Wahl , K J . 2008 . Base plate mechanics of the barnacle Balanus amphitrite (=Amphibalanus amphitrite) . Biofouling , 24 : 109 – 118 .
  • Rittschof , D and Costlow , J D . 1989 . Bryozoan and barnacle settlement in relation to initial surface wettability: a comparison of laboratory and field studies . Scientia Mar. , 53 : 411 – 416 .
  • Schmidt , D , Shah , D and Giannelis , E P . 2000 . New advances in polymer/layered silicates nanocomposites . Curr Opin Solid State Mater Sci. , 6 : 205 – 212 .
  • Schmidt , D L , Brady , R F , Lam , K , Schmidt , D C and Chaudhury , M K . 2004 . Contact angle hysteresis, adhesion and marine biofouling . Langmuir. , 20 : 2830 – 2836 .
  • Schultz , M P . 2007 . Effects of coating roughness and biofouling on ship resistance and powering . Biofouling , 23 : 331 – 341 .
  • Schultz , M P , Finlay , J A , Callow , M E and Callow , J A . 2000 . A turbulent channel flow apparatus for the determination of the adhesion strength of microfouling organisms . Biofouling , 15 : 243 – 251 .
  • Schultz , M P , Finlay , J A , Callow , M E and Callow , J A . 2003 . Three models to relate detachment of low form fouling at laboratory and ship scale . Biofouling , 19 ( Suppl ) : 17 – 26 .
  • Schumacher , J F , Aldred , N , Callow , M E , Finlay , J A , Callow , J A , Clare , A S and Brennan , A B . 2007a . Species-specific engineered antifouling topographies: correlations between the settlement of algal zoospores and barnacle cyprids . Biofouling , 23 : 307 – 317 .
  • Schumacher , J F , Carman , M L , Estes , T G , Feinberg , A W , Wilson , L H , Callow , M E , Callow , J A , Finlay , J A and Brennan , A B . 2007b . Engineered antifouling microtopographies––effect of feature size, geometry, and roughness on settlement of zoospores of the green alga Ulva . Biofouling , 23 : 55 – 62 .
  • Singer , I L , Kohl , J G and Patterson , M . 2000 . Mechanical aspects of silicone coatings for hard foulant control . Biofouling , 16 : 301 – 309 .
  • Stein , J , Truby , K , Darkangelo-Wood , C , Takemori , M , Vallance , M , Swain , G , Kavanagh , C , Kovach , B , Schultz , M Wiebe , D . 2003 . Structure–property relationships of silicone biofouling-release coatings: effect of silicone network architecture on pseudobarnacle attachment strengths . Biofouling , 19 : 87 – 94 .
  • Sun , M H , Luo , C X , Xu , L P , Ji , H , Qi , O Y and Yu , D P . 2005 . Artificial lotus leaf by nanocasting . Langmuir. , 21 : 5549 – 5554 .
  • Swain , G E . 1999 . Redefining antifouling coatings . Paint Coat Eur. , July 1999 : 18 – 25 .
  • Tai , N H , Yeh , M K and Liu , J H . 2004 . Enhancement of the mechanical properties of carbon nanotube/phenolic composites using a carbon nanotube network as the reinforcement . Carbon. , 42 : 2774 – 2777 .
  • Townsin , R L . 2003 . The ship hull fouling penalty . Biofouling , 19 ( Suppl ) : 9 – 15 .
  • Wendt , D E , Kowalke , G L , Kim , J and Singer , I L . 2006 . Factors that influence coatings performance: the effect of coating thickness on basal plate morphology, growth and critical removal stress of the barnacle Balanus amphitrite . Biofouling , 22 : 1 – 9 .
  • Yaobang , Z , Wencheng , F , Lu , W and Xiaobo , L . 2004 . Processing and property of MWNT/HDPE composite . Carbon. , 42 : 271 – 277 .
  • Zhang , Z H , Muller , R and Froelich , D . 1989 . Determination of crosslinking density of polymer networks by mechanical data in simple extension and by swelling degree at equilibrium . Polymer. , 30 : 2060 – 2062 .
  • Zhao , G and Deng , F . 2005 . Electroless plating of Ni-P-CNTs composite coating . Key Eng Mater. , 280–283 : 1445 – 1448 .

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below: