Microstructure, mechanical properties, and reinforcement mechanism of carbide toughened ZrC-based ultra-high temperature ceramics: A review

, , ORCID Icon, , , & show all
Pages 729-748 | Received 21 Aug 2021, Accepted 23 Nov 2021, Published online: 13 Jan 2022

References

  • Zhang YY, Yu LH, Fu, T et al. Microstructure and oxidation resistance of Si-MoSi2 ceramic coating on TZM (Mo-0.5Ti-0.1Zr-0.02C) alloy at 1500 °C Surf Coat Tech. 2022;431:128037.
  • Zweben C. Advanced composites for aerospace applications: a review of current status and future prospects. Composites. 1981;12(4):235–240.
  • Zhang X, Fu T, Cui KK, et al. Coatings the Protection, challenge, and prospect of anti-oxidation coating on the surface of niobium alloy. Coatings. 2021;11(7):742.
  • Monteverde F, Bellosi A, Scatteia L. Processing and properties of ultra-high temperature ceramics for space applications. Mat Sci Eng A Struct. 2008;485(1–2):415–421.
  • Fu T, Cui KK, Zhang YY, et al. Oxidation protection of tungsten alloys for nuclear fusion applications: a comprehensive review. J Alloy Compd. 2021;884:161057.
  • Fu T, Cui KK, Zhang YY, et al. Microstructure and oxidation behavior of anti-oxidation coatings on Mo-based alloys through HAPC process: a review. Coatings. 2021;11(8):883.
  • Wang J, Zhang YY, Cui KK, et al. Pyrometallurgical recovery of zinc and valuable metals from electric arc furnace dust – a review. J Clean Prod. 2021;298:126788.
  • Mao HB, Shen FQ, and Zhang YY, et al. Microstructure and Mechanical Properties of Carbide Reinforced TiC-Based Ultra-High Temperature Ceramics: A Review. Coatings. 2021;11:1444.
  • Squire TH, Marschall J. Material property requirements for analysis and design of UHTC components in hypersonic applications. J Eur Ceram Soc. 2010;30(11):2239–2251.
  • Blakey-Milner B, Gradl P, Snedden G, et al. Metal additive manufacturing in aerospace: a review. Mater Des. 2011;209:110008.
  • Fahrenholtz WG, Hilmas GE. Ultra-high temperature ceramics: materials for extreme environments. Scripta Mater. 2016;129:94–99.
  • Golla BR, Mukhopadhyay A, Basu B, et al. Review on ultra high temperature boride ceramics. Prog Mater Sci. 2020;111:100651.
  • He Z, Fu J. 3D characterization of the SiC nanoparticle distribution in ZrB2-SiC ceramics with synchrotron X-ray nanoscale computed tomography. Ceram Int. 2021;47(9):12780–12788.
  • He LK, Sun YH, Meng QN, et al. Enhanced oxidation properties of ZrB2-SiC composite with short carbon fibers at 1600°C. Ceram Int. 2021;47(11):15438–15490.
  • Nasseri MM. Comparison of HfB2 and ZrB2 behaviors for using in nuclear industry. Ann Nucl Energy. 2018;114:603–606.
  • Liu HL, Liu JX, Bao WC, et al. Interface characteristics in ZrB2-based ceramics containing SiC and/or ZrC particles via hot-pressing sintering. Mater Charact. 2021;176:111144.
  • Zhang YY, Fu T, Cui KK, et al. Evolution of surface morphology, roughness and texture of tungsten disilicide coatings on tungsten substrate. Vacuum. 2021;191:110297.
  • Toozandehjani M, Kamarudin N, Dashtizadeh Z, et al. Conventional and advanced composites in aerospace industry: technologies revisited. J Aerospace Eng. 2018;5(1):9–15.
  • Justin JF, Jankowiak A. Ultra high temperature ceramics: densification, properties and thermal stability. High Temp Mat Pr-Isr. 2011;3:3–8.
  • Upadhya K, Yang JM, Hoffman W. Advanced materials for ultrahigh temperature structural applications above 2000 deg C. Am Ceram Soc Bull. 1997;76:23.
  • Jiang M, Zheng JW, Xiao HY, et al. A comparative study of the mechanical and thermal properties of defective ZrC, TiC and SiC. Sci Rep-Uk. 2017;7:9344.
  • Cui KK, Zhang YY, Fu T, et al. Effects of Cr2O3 content on microstructure and mechanical properties of Al2O3 matrix composites. Coatings. 2021;11(2):234.
  • Zhang YY, Cui KK, Fu T, et al. Formation of MoSi2 and Si/MoSi2 coatings on TZM (Mo-0.5Ti-0.1Zr-0.02C) alloy by hot dip silicon-plating method. Ceram Int. 2021;47(16):23053–23065.
  • Li Y, Li Q, Wang Z. Microstructures and mechanical properties of laminated ZrC-SiC composites with different SiC powders. Ceram Int. 2015;41(10):15255–15260.
  • Zhao J, Xue JX, Liu HT, et al. ZrC ceramics incorporated with different-sized SiC particles. Adv Appl Ceram. 2018;117(7):383–388.
  • Li JP, Meng SH, Wang ZB, et al. Study on ZrC-20vol.%SiCw ultrahigh temperature ceramics by hot pressing. Adv Mater Res. 2012;557-559:772–775.
  • Yan C, Liu R, Zhang C, et al. Mechanical behaviour and microstructure of Cf/ZrC, Cf/SiC and Cf/ZrC - SiC composites. Adv Appl Ceram. 2016;115(7):1–5.
  • Shimada S. TEM observation of the ZrC/ZrO2 interface formed by oxidation of ZrC single crystals. J Mater Synth Proces. 1998;6:191–195.
  • Kumashiro Y, Nagai Y, Kato H, et al. The preparation and characteristics of ZrC and TaC single crystals using an r.f. floating-zone process. J Mater Sci. 1981;16:2930–2933.
  • Porter IE, Knight TW, Dulude MC, et al. Design and fabrication of an advanced TRISO fuel with ZrC coating. Nucl Eng Des. 2013;259:180–186.
  • Zhang YY, Cui KK, Gao QJ, et al. Investigation of morphology and texture properties of WSi2 coatings on W substrate based on contact-mode AFM and EBSD. Surf Coat Tech. 2020;396:125966.
  • Zhang YY, Cui KK, Wang J, et al. Effects of direct reduction process on the microstructure and reduction characteristics of carbon-bearing nickel laterite ore pellets. Powder Technol. 2020;376:496–506.
  • Kim KS, Lee SH, Nguyen VQ, et al. Ablation characteristics of rocket nozzle using HfC-SiC refractory ceramic composite. Acta Astronaut. 2020;173:31–44.
  • Tao X, Liu L, Li W, et al. Ablation behaviour of C/C-ZrC composites in a solid rocket motor environment. Ceram Int. 2015;41(9):11793–11803.
  • Vernillo S, Giordano R, Vernillo I. Application of ZrC-coated tubes to the determination of aluminum in serum by graphite furnace atomic absorption spectroscopy. Microchem J. 1984;30:425–434.
  • Caccia M, Tabandeh-Khorshid M, Itskos G, et al. Sandhage, Ceramic-metal composites for heat exchangers in concentrated solar power plants. Nature. 2018;562:406–409.
  • Li C, Li L, Li J, et al. Fabrication and characterisation of viscose fibre with photoinduced heat-generating properties. Cellulose. 2019;26:1631–1640.
  • Atchison JS, Zeiger M, Tolosa A, et al. Electrospinning of ultrafine metal oxide/carbon and metal carbide/carbon nanocomposite fibers. Rsc Adv. 2015;5:35683–35692.
  • Xu J, Jiang S, Wang Y, et al. Photo-thermal conversion and thermal insulation properties of ZrC coated polyester fabric. Fiber Polym. 2017;18:1938–1944.
  • Chayeuski V, Zhylinski V, Cernashejus O, et al. Structural and mechanical properties of the ZrC/Ni-Nanodiamond coating synthesized by the PVD and electroplating processes for the cutting knifes. J Mater Eng Perform. 2018;28:1278–1285.
  • Song G, Wang Y, Zhou Y. The influence of ZrC particle content on the mechanical properties of tungsten matrix composites. Nonferr Metal Soc. 2001;53:47–51.
  • Cui KK, Fu T, Zhang YY, et al. Microstructure and mechanical properties of CaAl12O19 reinforced Al2O3-Cr2O3 composites. J Eur Ceram Soc. 2021;41(15):7935–7945.
  • Zhang YY, Yu LH, Fu, T et al. Microstructure evolution and growth mechanism of Si-MoSi2 composite coatings on TZM (Mo-0.5Ti-0.1Zr-0.02 C) alloy. J Alloy Compd. 2022;894:162403.
  • Cui KK, Zhang YY, Fu T, et al. Toughening mechanism of mullite matrix composites: a review. Coatings. 2020;10(7):672.
  • Feng L, Fahrenholtz WG, Hilmas GE. Effect of ZrB2 content on the densification, microstructure, and mechanical properties of ZrC-SiC ceramics. J Eur Ceram Soc. 2020;40(2):220–225.
  • Feng L, Fahrenholtz WG, Hilmas GE, et al. Densification, microstructure, and mechanical properties of ZrC-SiC ceramics. J Am Ceram Soc. 2019;102(10):5786–5795.
  • Yung DL, Hussainova I, Rodriguez MA, et al. Processing of ZrC-TiC composites by SPS. Key Eng Mat. 2016;674:94–99.
  • Liang M, Li F, Ma X, et al. Syntheses of ZrC-SiC nanopowder via sol-gel method. Ceram Int. 2016;42(1):1345–1351.
  • Zhao L, Jia D, Duan X, et al. Low temperature sintering of ZrC-SiC composite. J Alloy Compd. 2011;509(41):9816–9820.
  • Antou G, Ohin MD, Lucas R, et al. Thermomechanical properties of a spark plasma sintered ZrC-SiC composite obtained by a precursor derived ceramic route. Mat Sci Eng A Struct. 2015;643:1–11.
  • Sciti D, Guicciardi S, Nygren M. Spark plasma sintering and mechanical behaviour of ZrC-based composites. Scripta Mater. 2008;59(6):638–641.
  • Wang XG, Zhang GJ, Xue JX, et al. Reactive hot pressing of ZrC–SiC ceramics at low temperature. J Am Ceram Soc. 2013;96(1):32–36.
  • Yung DL, Cygan S, Antonov M, et al. Ultra high-pressure spark plasma sintered ZrC-Mo and ZrC-TiC composites. Int J Refract Met H. 2016;61:201–206.
  • Acicbe RB, Goller G. Densification behavior and mechanical properties of spark plasma-sintered ZrC-TiC and ZrC-TiC-CNT composites. J Mater Sci. 2013;48:2388–2393.
  • Ocak BC, Yavas B, Akin I, et al. Spark plasma sintered ZrC-TiC-GNP composites: solid solution formation and mechanical properties. Ceram Int. 2018;44(2):2336–2344.
  • Zhao J, Zou J, Man ZY, et al. Dopant effects on high temperature mechanical properties of zirconium carbide ceramics. Adv Appl Ceram. 2015;114:338–343.
  • Kinloch AJ, Mohammed RD, Taylor AC, et al. Toughening mechanisms of nanoparticle-modified epoxy polymers. Polymer. 2007;48(2):530–541.
  • Jeong Y, Choa Y, Niihara K. Strengthening and toughening mechanisms of ceramic nanocomposites. J Am Ceram Soc. 1998;81(6):1453–1460.
  • Nalla RK, Kinney JH, Ritchie RO. Effect of orientation on the in vitro fracture toughness of dentin: the role of toughening mechanisms. Biomaterials. 2003;24(22):3955–3968.
  • Liu H, Huang C, Qin H, et al. Research evolution on the strengthening and toughening mechanisms of nano-scale composite ceramics. Poeder Metall. 2004;22:98–103.
  • Zhong J, Huang C, Nie Q. Effect of nano-scale TiC on microstructure and mechanical properties of nano-scale zirconia toughening alumina matrix ceramic tool materials. Tool Engineering. 2011;45:27–30.
  • Labronici M, Ishida H. Toughening composites by fiber coating: a review. Compos Interfaces. 1994;2(3):199–234.
  • Helmuth J, Schalek RL, Drzal LT. Correlation of the mechanical properties to the fiber-matrix adhesion of Nextel 312™ fiber/BN/Blackglas™ composites. Compos Interfaces. 2003;10(2–3):119–138.
  • Wu WJ, Sun ZG, Niu XM, et al. Simulating the corrosion and microstructure evolution of SiCf/PyC/SiCm composites in a humid oxygen environment. Compos Interfaces. 2021. doi:https://doi.org/10.1080/09276440.2020.1858225.
  • Fang GW, Gao XG, Song YD. XFEM analysis of crack propagation in fiber-reinforced ceramic matrix composites with different interphase thicknesses. Compos Interfaces. 2020;27(3):327–340.
  • Fu SL, Wang YX, Niu FX, et al. Preparation and characterization of t-BN coatings on the surface of carbon fibers. Compos Interfaces. 2019;26(6):479–492.
  • Xu ZK, Sun XH, Xiong KZ. A review of the research progress on the interface between oxide fiber and oxide ceramic matrix. Ceram Int. 2021;47(5):5896–5908.
  • Li Q, Dong S, Wang Z, et al. Fabrication and properties of 3-D Cf/ZrC-SiC composites via in-situ reaction. Ceram Int. 2014;40:2483–2488.
  • Li Q, Dong S, Wang Z, et al. Fabrication of a ZrC-SiC matrix for ceramic matrix composites via in-situ reaction and its application. Ceram Int. 2013;39(1):877–881.
  • Cheng Y, Liu C, Hu P, et al. Using PyC coated short chopped carbon fiber to tackle the dilemma between toughness and strength of ZrC-SiC. Ceram Int. 2019;45(1):503–509.
  • Yan C, Liu R, Zhang C, et al. Effect of PyC interphase thickness on mechanical and ablation properties of 3D Cf/ZrC-SiC composite. Ceram Int. 2016;42(11):12756–12762.
  • Wang D, Dong S, Zhou H, et al. Fabrication and microstructure of 3D Cf /ZrC-SiC composites: through RMI method with ZrO2 powders as pore-making agent. Ceram Int. 2016;42(1):6720–6727.
  • Belmonte M, Nistal A, Boutbien P, et al. Toughened and strengthened silicon carbide ceramics by adding graphene-based fillers. Scripta Mater. 2016;113:127–130.
  • Yadhukulakrishnan GB, Karumuri S, Rahman A, et al. Spark plasma sintering of graphene reinforced zirconium diboride ultra-high temperature ceramic composites. Ceram Int. 2013;39(6):6637–6646.
  • Cheng Y, Hu P, Zhou S, et al. Using macroporous graphene networks to toughen ZrC-SiC ceramic. J Eur Ceram Soc. 2018;38(11):3752–3758.
  • Hou C, Zhang S, Ma Z, et al. Effects of SiC fibers and laminated structure on mechanical properties of Ti-Al laminated composites. Materials. 2021;14(6):1323.
  • You B, Liang D, Hao P, et al. Deployment dynamical behavior of planetary rover mast mechanism considering geometric nonlinearity and laminated structure characteristics. Arch Appl Mech. 2020;90:1605–1623.
  • Gao QY, Li SX, Su YS, et al. Grain coarsening of nano laminated structure in martensite steel under sliding wear. Tribol Int. 2020;151:106381.
  • Li D, Qiao G, Jin Z. R-curve behavior of laminated SiC/BN ceramics. Ceram Int. 2004;30(2):213–217.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.