249
Views
9
CrossRef citations to date
0
Altmetric
Original Articles

Effect of Compressive Deformation on Wear Property of Extruded ZK60 Magnesium Alloy

, , , &
Pages 1-7 | Received 16 Apr 2017, Accepted 31 Dec 2017, Published online: 25 Oct 2018

References

  • Baldwin, K. R. and Bray, D. J. (1996), “Corrosion Behaviour of Some Vapour Deposited Magnesium Alloys,” Materials Science and Technology, 12(11), pp 929–944.
  • Lu, L. W., Hu, S. H., and Liu, L. F. (2016), “High Speed Cutting of AZ31 Magnesium Alloy,” Journal of Magnesium Alloys, 4(2), pp 128–134.
  • Tong, L. B., Zheng, M. Y., and Kamado, S. (2015), “Reducing the Tension–Compression Yield Asymmetry of Extruded Mg-Zn-Ca Alloy via Equal Channel Angular Pressing,” Journal of Magnesium Alloys, 3(4), pp 302–308.
  • An, J., Li, R. G., and Lu, Y. (2008), “Dry Sliding Wear Behavior of Magnesium Alloys,” Wear, 265(1), pp 97–104.
  • Mehta, D. S., Masood, S. H., and Song, W. Q. (2004), “Investigation of Wear Properties of Magnesium and Aluminum Alloys for Automotive Applications,” Journal of Materials Processing Technology, 155–156(6), pp 1526–1531.
  • Christian, J. W. and Mahajan, S. (1995), “Deformation Twinning,” Progress in Materials Science, 39(1–2), pp 1–157.
  • Zhang, H. and Huang, G. S. (2013), “Enhanced Mechanical Properties of AZ31 Magnesium Alloy Sheets Processed by Three-Directional Rolling,” Journal of Alloys and Compounds, 575(8), pp 408–413.
  • Barnett, M. R. (2007), “Twinning and the Ductility of Magnesium Alloys: Part II. Contraction Twins,” Materials Science and Engineering A, 464(1), pp 8–16.
  • Park, S. H., Hong, S. G., and Lee, C. S. (2010), “Role of Initial {10-12} Twin in the Fatigue Behavior of Rolled Mg-3Al-1Zn Alloy,” Scripta Materialia, 62(9), pp 666–669.
  • Zhang, H. and Huang, G. S. (2012), “Improved Formability of Mg-3Al-1Zn Alloy by Pre-Stretching and Annealing,” Scripta Materialia, 67(5), pp 495–498.
  • Song, B. and Xin, R. L. (2012), “Improving and Compressive Properties of Magnesium Alloy Plates by Pre–Cold Rolling,” Scripta Materialia, 66(12), pp 1061–1064.
  • Xu, J., Wang, X. W., and Zhu, X. C. (2013), “Dry Sliding Wear of an AZ31 Magnesium Alloy Processed by Equal-Channel Angular Pressing,” Journal of Materials Science, 48(11), pp 4117–4127.
  • Hu, H. J., Fan, J. Z., and Wang, H. (2015), “Dry Sliding Wear Behavior of ES-Processed AZ31B Magnesium Alloy,” Russian Journal of Non-Ferrous Metals, 56(4), pp 392–398.
  • Kato, H., Todaka, Y., and Umemoto, M. (2015), “Sliding Wear Behavior of Sub-Microcrystalline Pure Iron Produced by High-Pressure Torsion Straining,” Wear, 336–337(1), pp 58–68.
  • Edalati, K., Ashida, M., and Horita, Z. J. (2014), “Wear Resistance and Tribological Features of Pure Aluminum and Al-Al2O3 Composites Consolidated by High-Pressure Torsion,” Wear, 310(1–2), pp 83–89.
  • Habibnejad-Korayem, M., Mahmudi R., and Ghasemi, H. M. (2010), “Tribological Behavior of Pure Mg and AZ31 Magnesium Alloy Strengthened by Al2O3 Nano-Particles,” Wear, 268(3–4), pp 405–412.
  • Bi, G. L., Li, Y. D., and Huang, X. F. (2015), “Dry Sliding Wear Behavior of an Extruded MgeDyeZn Alloy with Long Period Stacking Ordered Phase,” Journal of Magnesium Alloys, 3, pp 63–69.
  • Lopez, A. J., Rodrigo, P., and Torres, B. (2011), “Dry Sliding Wear Behaviour of ZE41A Magnesium Alloy,” Wear, 271(11), pp 2836–2844.
  • Zafari, A., Ghasemi, H. M., and Mahmudi, R. (2013), “Effect of Rare Earth Elements Addition on the Tribological Behavior of AZ91D Magnesium Alloy at Elevated Temperatures,” Wear, 303(1–2), pp 98–108.
  • Taltavull, C., Torres, B., and Lopez, A. J. (2013), “Dry Sliding Wear Behavior of AM60B Magnesium Alloy,” Wear, 301(1–2), pp 615–625.
  • Zafari, A., Ghasemi, H. M., and Mahmudi, R. (2014), “An Investigation on the Tribological Behavior of AZ91 and AZ91 + 3wt% RE Magnesium alloys at Elevated Temperatures,” Materials & Design, 54(2), pp 544–552.
  • Jiang, L. Jonas, J. J., and Luo, A. A. (2007), “Influence of {10-12} Extension Twinning on the Flow Behavior of AZ31Mg Alloy,” Materials Science and Engineering A, 445–446(6), pp 302–309.
  • Xin, Y. C., Wang, M. Y., Zeng, Z., Nie, M. G., and Liu, Q. (2012), “Strengthening and Toughening of Magnesium Alloy by {1012} Extension Twins,” Scripta Materialia, 66(1), pp 25–28.
  • Rao, R. N., Das, S., Mondal, D. P., and Dixit, G. (2009), “Dry Sliding Wear Behaviour of Cast High Strength Aluminium Alloy (Al-Zn-Mg) and Hard Particle Composites,” Wear, 267(9–10), pp 1688–1695.
  • Ghazali, M. J., Rainforth, W. M., and Jones, H. (2007), “The Wear of Wrought Aluminium Alloys under Dry Sliding Conditions,” Tribology International, 40(2), pp 160–169.
  • Shanthi, M., Lim C. Y. H., and Lu, L. (2007), “Effects of Grain Size on the Wear of Recycled AZ91Mg,” Tribology International, 40(2), pp 335–338.
  • Dwivedi, D. K., Arjun, T. S., Thakur, P., Vaidya, H., and Singh, K. (2004), “Sliding Wear and Friction Behaviour of Al-18% Si-0.5% Mg Alloy,” Journal of Materials Processing Technology, 152(3), pp 323–328.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.