References
- Wang, Q.-Y., Bai, S.-L., and Liu, Z.-D. (2014), “Study on Cavitation Erosion–Corrosion Behavior of Mild Steel under Synergistic Vibration Generated by Ultrasonic Excitation,” Tribology Transactions, 57(4), pp 603–612. doi:https://doi.org/10.1080/10402004.2014.890264
- Kasolang, S. and Dwyer-Joyce, R. S. (2008), “Observations of Film Thickness Profile and Cavitation around a Journal Bearing Circumference,” Tribology Transactions, 51(2), pp 231–245. doi:https://doi.org/10.1080/10402000801947717
- Sreedhar, B. K., Albert, S. K., and Pandit, A. B. (2017), “Cavitation Damage: Theory and Measurements—A Review,” Wear, 372–373, pp 177–196. doi:https://doi.org/10.1016/j.wear.2016.12.009
- Liu, F., Wang, J., Chen, D., Xu, Y., and Zhao, M. (2010), “The Cavitation Erosion of the 45# Carbon Steels Implanted with Titanium and Nitrogen,” Tribology Transactions, 53(2), pp 239–243.
- Meili, S., Zhiming, Z., Xiaoyang, C., Wen, W., Kai, M., and Sun, D. C. (2008), “Experimental Study of Cavitation in an Oscillatory Oil Squeeze Film,” Tribology Transactions, 51(3), pp 341–350. doi:https://doi.org/10.1080/10402000701793989
- Rao, T. V. V. L. N. and Sawicki, J. T. (2002), “Linear Stability Analysis for a Hydrodynamic Journal Bearing Considering Cavitation Effects,” Tribology Transactions, 45(4), pp 450–456. doi:https://doi.org/10.1080/10402000208982573
- Ai, W., Lo, K. H., and Kwok, C. T. (2019), “Cavitation Erosion of a Spinodally Decomposed Wrought Duplex Stainless Steel in a Benign Environment,” Wear, 424–425, pp 111–121.
- Prasanna, G. L., Tanya, B., Subbiah, R., and Vinod Kumar, V. (2020), “Effect of Nitriding on Duplex Stainless Steel—A Review,” Materials Today: Proceedings, 26, pp 950–955.
- Varghese, P., Vetrivenden, E., Kumar Dash, M., Ningshen, S., Kamaraj, M., and Mudali, U. K. (2018), “Weld Overlay Coating of Inconel 617 M on Type 316 L Stainless Steel by Cold Metal Transfer Process,” Surface and Coatings Technology, 357(9), pp 1004–1013.
- Sathirachinda, N., Pettersson, R., and Pan, J. (2009), “Depletion Effects at Phase Boundaries in 2205 Duplex Stainless Steel Characterized with SKPFM and TEM/EDS,” Corrosion Science, 51(8), pp 1850–1860.
- Yang, Y. H., Yan, B., Wang, J., and Yin, J. L. (2011), “The Influence of Solution Treatment Temperature on Microstructure and Corrosion Behavior of High Temperature Ageing in 25% Cr Duplex Stainless Steel,” Journal of Alloys and Compounds, 509(36), pp 8870–8879.
- Ou, M., Ma, Y., Hao, X., Wan, B., Liang, T., and Liu, K. (2017), “Effect of Solution Annealing on Microstructure and Mechanical Properties of a Ni-Cr-W-Fe Alloy,” Journal of Materials Science & Technology, 33(11), pp 1300–1307.
- Mampuya, M. B., Umba, M. C., Mutombo, K., and Olubambi, P. A. (2020 ), “Effect of Heat Treatment on the Microstructure of Duplex Stainless Steel 2205,” Materials Today: Proceedings, 38, pp 1107–1112.
- Wang, Z. and Zhu, J. (2004), “Correlation of Martensitic Transformation and Surface Mechanical Behavior with Cavitation Erosion Resistance for Some Iron-Based Alloys,” Wear, 256(11), pp 1208–1213. doi:https://doi.org/10.1016/j.wear.2003.10.008
- Nair, R. B., Arora, H. S., Mukherjee, S., Singh, S., Singh, H., and Grewal, H. S. (2018), “Exceptionally High Cavitation Erosion and Corrosion Resistance of a High Entropy Alloy,” Ultrasonics Sonochemistry, 41, pp 252–260. doi:https://doi.org/10.1016/j.ultsonch.2017.09.044
- Zhang, J., Hu, X.-j., Lin, P., and Chou, K. (2018), “Effect of Solution Annealing on the Microstructure Evolution and Corrosion Behavior of 2205 Duplex Stainless Steel,” Materials and Corrosion, 70(4), pp 1–12. doi:https://doi.org/10.1002/maco.201810536
- Liu, C.-P., Chang, S.-J., Liu, Y.-F., and Su, J. (2020), “Corrosion-Induced Degradation and Its Mechanism Study of Cu–Al Interface for Cu-Wire Bonding under HAST Conditions,” Journal of Alloys and Compounds, 825, pp 154046. doi:https://doi.org/10.1016/j.jallcom.2020.154046
- Eivazzadeh-Keihan, R., Taheri-Ledari, R., Khosropour, N., Dalvand, S., Maleki, A., Mousavi-Khoshdel, S. M., and Sohrabi, H. (2020), “Fe3O4/GO@melamine-ZnO Nanocomposite: A Promising Versatile Tool for Organic Catalysis and Electrical Capacitance,” Colloids and Surfaces A: Physicochemical and Engineering Aspects, 587, pp 124335. doi:https://doi.org/10.1016/j.colsurfa.2019.124335
- Chiu, K., Cheng, F., and Man, H. (2005), “Evolution of Surface Roughness of Some Metallic Materials in Cavitation Erosion,” Ultrasonics, 43(9), pp 713–716. doi:https://doi.org/10.1016/j.ultras.2005.03.009
- Long, X., Yao, H., and Zhao, J. (2009), “Investigation on Mechanism of Critical Cavitating Flow in Liquid Jet Pumps under Operating Limits,” International Journal of Heat & Mass Transfer, 52(9–10), pp 2415–2420.
- Xu, H. and Dong, Q. (2019), “Cavitation Erosion Behavior of Duplex Stainless Steel under High-Pressure Jet,” Materials Science Forum, 950, pp 3–9. doi:https://doi.org/10.4028/www.scientific.net/MSF.950.3
- Al-Hashem, A., Caceres, P. G., and Abdullah, A. (1997), “Cavitation Corrosion of Duplex Stainless Steel in Seawater,” Corrosion, 53(2), pp 103–113. doi:https://doi.org/10.5006/1.3280438
- Guo, L. Q., Qin, S. X., Yang, B. J., Liang, D., and Qiao, L. J. (2017), “Effect of Hydrogen on Semiconductive Properties of Passive Film on Ferrite and Austenite Phases in a Duplex Stainless Steel,” Scientific Reports, 7(1), pp 3317. doi:https://doi.org/10.1038/s41598-017-03480-8
- Neville, A. and Hodgekiess, T. (2013), “Study of Effect of Liquid Corrosivity in Liquid–Solid Impingement on Cast Iron and Austenitic Stainless Steel,” British Corrosion Journal, 12(3), pp 197–205. doi:https://doi.org/10.1179/bcj.1997.32.3.197
- Chen, M., Jiang, C., Xu, Z., and Ji, V. (2019), “Surface Layer Characteristics of SAF2507 Duplex Stainless Steel Treated by Stress Shot Peening,” Applied Surface Science, 481, pp 226–233.