An Investigation Into the Synergistic Effect of CAPVD Cr/CrN Nanolayered Coating Deposition and Hard-Anodizing Methods on Fretting Fatigue Life of 7075-T6 Aluminum Alloy

, &
Pages 683-696 | Received 24 Jul 2022, Accepted 28 May 2023, Published online: 26 Jun 2023

References

  • Shen, L. J., Lohrengel, A., and Schäfer, G. (2013), “Plain–Fretting Fatigue Competition and Prediction in Spline Shaft–Hub Connection,” International Journal of Fatigue, 52, pp 68–81. doi:10.1016/j.ijfatigue.2012.11.012
  • Chehrazi, A., Walbridge, S., Mohareb, S., Goldack, A., and Schlaich, M. (2020), “Probabilistic Fretting Fatigue Analysis of Bridge Stay Cables at Saddle Supports,” Structural Engineering International, 30(4), pp 571–579. doi:10.1080/10168664.2019.1661332
  • Zhao, L., He, X., Xing, B., Lu, Y., Gu, F., and Ball, A. (2015), “Influence of Sheet Thickness On Fatigue Behavior and Fretting of Self-Piercing Riveted Joints in Aluminum Alloy 5052,” Materials & Design, 87, pp 1010–1017. doi:10.1016/j.matdes.2015.08.121
  • Vantadori, S., Abbasi, F., Zanichelli, A., Leonetti, D., Pio Pucillo, G., and Hossein Majzoobi, G. (2022), “Influence of Normal Load Frequency on Fretting Fatigue Behaviour by a Critical Plane-Based Approach,” International Journal of Fatigue, 158, p 106724. doi:10.1016/j.ijfatigue.2022.106724
  • Almeida, G. M. J., Pessoa, G. C. V., Cardoso, R. A., Castro, F. C., and Araújo, J. A. (2020), “Investigation of Crack Initiation Path in AA7050-T7451 Under Fretting Conditions,” Tribology International, 144, p 106103. doi:10.1016/j.triboint.2019.106103
  • Majzoobi, G. H., Nemati, J., Novin Rooz, A. J., and Farrahi, G. H. (2009), “Modification of Fretting Fatigue Behavior of AL7075–T6 Alloy by the Application of Titanium Coating Using IBED Technique and Shot Peening,” Tribology International, 42(1), pp 121–129. doi:10.1016/j.triboint.2008.05.006
  • Majzoobi, G. H., and Ahmadkhani, A. R. (2010), “The effects of multiple re-shot peening on fretting fatigue behavior of Al7075-T6,” Surface and Coatings Technology 205(1), pp 102–109. doi:10.1016/j.surfcoat.2010.06.014
  • Mitterer, C. (2014), PVD and CVD Hard Coatings, pp 449–467. Elsevier: Oxford.
  • Gilewicz, A., Chmielewska, P., Murzynski, D., Dobruchowska, E., and Warcholinski, B. (2016), “Corrosion Resistance of CrN and CrCN/CrN Coatings Deposited Using Cathodic Arc Evaporation in Ringer's and Hank's Solutions,” Surface and Coatings Technology, 299, pp 7–14. doi:10.1016/j.surfcoat.2016.04.069
  • Chang, Y.-Y., Wang, D.-Y., and Hung, C.-Y. (2005), “Structural and Mechanical Properties of nanolayered TiAlN/CrN Coatings Synthesized by a Cathodic Arc Deposition Process,” Surface and Coatings Technology, 200(5), pp 1702–1708. doi:10.1016/j.surfcoat.2005.08.088
  • Vengesa, Y., Fattah-alhosseini, A., Elmkhah, H., and Imantalab, O. (2022), “Influence of Post-Deposition Annealing Temperature on Morphological, Mechanical and Electrochemical Properties of CrN/CrAlN Multilayer Coating Deposited by Cathodic Arc Evaporation–Physical Vapor Deposition Process,” Surface and Coatings Technology, 432, p 128090. doi:10.1016/j.surfcoat.2022.128090
  • Mansoor, N. S., Fattah-Alhosseini, A., Elmkhah, H., and Shishehian, A. (2020), “Comparison of the Mechanical Properties and Electrochemical Behavior of TiN and CrN Single-Layer and CrN/TiN Multi-Layer Coatings Deposited by PVD Method on a Dental Alloy,” Materials Research Express, 6(12), p 126433. doi:10.1088/2053-1591/ab640d
  • Anders, A. (2010), Unfiltered and Filtered Cathodic Arc Deposition, pp 466–531. William Andrew Publishing: Boston.
  • Bull, S. J., and Jones, A. M. (1996), “Multilayer Coatings for Improved Performance,” Surface and Coatings Technology, 78(1), pp 173–184. doi:10.1016/0257-8972(94)02407-3
  • Borawski, B., Singh, J., and Todd, J. (2011), “Multi-Layer Coating Design Architecture for Optimum Particulate Erosion Resistance,” Wear, 271, pp 2782–2792. doi:10.1016/j.wear.2011.05.035
  • Anders, A. (2008), Cathodic Arcs: From Fractal Spots to Energetic Condensation. Springer: New York. ISBN 978–0387791074.
  • Pogrebnjak, A., Beresnev, V. M., Bondar, O., Postolnyi, B., Załęski, K., Coy, E., Jurga, S., Lisovenko, M., Konarski, P., Rebouta, L., and Araujo, J. (2018), “Superhard CrN/MoN Coatings With Multilayer Architecture,” Materials & Design, 153. doi:10.1016/j.matdes.2018.05.001
  • Frank, F., Kainz, C., Tkadletz, M., Czettl, C., Pohler, M., and Schalk, N. (2022), “Microstructural and Micro-Mechanical Investigation of Cathodic Arc Evaporated ZrN/TiN Multilayer Coatings With Varying Bilayer Thickness,” Surface and Coatings Technology, 432, p 128070. doi:10.1016/j.surfcoat.2021.128070
  • Sui, X., Liu, J., Zhang, S., Yang, J., and Hao, J. (2018), “Microstructure, Mechanical and Tribological Characterization of CrN/DLC/Cr-DLC Multilayer Coating With Improved Adhesive Wear Resistance,” Applied Surface Science, 439, pp 24–32. doi:10.1016/j.apsusc.2017.12.266
  • Tritremmel, C., Daniel, R., Rudigier, H., Polcik, P., and Mitterer, C. (2014), “Mechanical and Tribological Properties of Al-Ti-N/Al-Cr-B-N Multilayer Films Synthesized by Cathodic Arc Evaporation,” Surface and Coatings Technology, 246, pp 57–63. doi:10.1016/j.surfcoat.2014.03.005
  • Ottone, C., Laurenti, M., Bejtka, K., Sanginario, A., and Valentina, C. (2014), “The Effects of the Film Thickness and Roughness in the Anodization Process of Very Thin Aluminum Films,” Journal of Materials Science & Nanotechnology, 1, p S107.
  • Mattox, D. M. (2010), The “Good” Vacuum (Low Pressure) Processing Environment, 2nd ed., pp 73–145. William Andrew Publishing: Boston,
  • Majzoobi, G. H., and Jaleh, M. (2007), “Duplex Surface Treatments on AL7075-T6 Alloy Against Fretting Fatigue Behavior by Application Of Titanium Coating Plus Nitriding,” Materials Science and Engineering: A, 452–453, pp 673–681. doi:10.1016/j.msea.2006.11.007
  • Liu, W., Xia, H., Liu, Y., Song, Z., and Xu, X. (2013), “The Performances of a Thermally Sprayed Fe/Ni Composite Coating to Resist Fretting Fatigue Under Rotational Bending Loads,” Surface and Coatings Technology, 217, pp 58–63. doi:10.1016/j.surfcoat.2012.11.072
  • Tang, C.-B., Liu, D.-X., Tang, B., Zhang, X.-H., Qin, L., and Liu, C.-S. (2016), “Influence of Plasma Molybdenizing and Shot-Peening on Fretting Damage Behavior of Titanium Alloy,” Applied Surface Science, 390, pp 946–958. doi:10.1016/j.apsusc.2016.08.146
  • Vidakis, N., Antoniadis, A., and Bilalis, N. (2003), “The VDI 3198 Indentation Test Evaluation of a Reliable Qualitative Control For Layered Compounds,” Journal of Materials Processing Technology, 143–144, pp 481–485. doi:10.1016/S0924-0136(03)00300-5
  • Jönsson, B., and Hogmark, S. (1984), “Hardness Measurements of Thin Films,” Thin Solid Films, 114(3), pp 257–269. doi:10.1016/0040-6090(84)90123-8
  • Jasempoor, F., Elmkhah, H., Imantalab, O., and Fattah-Alhosseini, A. (2022), “Improving the Mechanical, Tribological, and Electrochemical Behavior of AISI 304 Stainless Steel by Applying CrN Single Layer and Cr/CrN Multilayer Coatings,” Wear, 504–505, pp 204425. doi:10.1016/j.wear.2022.204425
  • Majzoobi, G. H., Azadikhah, K., and Nemati, J. (2009), “The Effects of Deep Rolling and Shot Peening on Fretting Fatigue Resistance of Aluminum-7075-T6,” Materials Science and Engineering: A, 516, 1, pp 235–247. doi:10.1016/j.msea.2009.03.020
  • Fang, J., Han, Q., Cui, H., Lei, X., Yan, X., Mu, Q., Xu, J., and Shi, H. (2023), “Fretting Fatigue Experiment and Polycrystal Plasticity Simulation in Ni-Based Superalloy at Room Temperature and 650 °C,” International Journal of Fatigue, 168, pp 107460. doi:10.1016/j.ijfatigue.2022.107460
  • Abbasi, F., Majzoobi, G., and Mendiguren, J. (2020), “A Review of the Effects of Cyclic Contact Loading on Fretting Fatigue Behavior,” Advances in Mechanical Engineering, 12(9), p 1687814020957175. doi:10.1177/1687814020957175
  • Vingsbo, O., and Söderberg, S. (1988), “On Fretting Maps,” Wear, 126(2), pp 131–147. doi:10.1016/0043-1648(88)90134-2
  • Nishioka, K., and Hirakawa, K. (1969), “Fundamental Investigations of Fretting Fatigue: Part 2, Fretting Fatigue Testing Machine and Some Test Results,” Bulletin of JSME, 12(50), pp 180–187. doi:10.1299/jsme1958.12.180
  • Chun, S.-Y., Lee, S.-J., Lee, C.-H., and Chayahara, A. (2005), Nanometer-Ranged Metallic Coatings by Noble Pulsed Cathodic Arc Deposition, pp 83–86. Elsevier Science Ltd: Oxford.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.