The effects of temperature and agitation speed on the leaching behaviors of tin and bismuth from spent lead free solder in nitric acid leach solution

, , &
Pages 213-218 | Received 11 Apr 2015, Accepted 03 May 2015, Published online: 19 Jun 2015

References

  • Felton, L. E. , Raeder, C. H. , & Knorr, D. B. (1993). The Properties of Tin-Bismuth Alloy Solders. JOM, 45, 28–32. doi: 10.1007/BF03222377.
  • Ficeriová, J. , Baláž, P. , & Villachica, C. L. (2005). Thiosulfate leaching of silver, gold and bismuth from a complex sulfide concentrates. Hydrometallurgy, 77, 35–39. doi: 10.1016/j.hydromet.2004.09.010.
  • Kim, S. , Lee, J. , Lee, K. , Yoo, K. , & Alorro, R. D. (2014). Separation of tin, silver and copper from waste Pb-free solder using hydrochloric acid leaching with hydrogen peroxide. Materials Transactions, 55, 1885–1889. doi: 10.2320/matertrans.M2014289.
  • Ma, H. , & Suhling, J. C. (2009). A review of mechanical properties of lead-free solders for electronic packaging. Journal of Materials Science, 44, 1141–1158. doi: 10.1007/s10853-008-3125-9.
  • Pan, J. , Wang, J. , & Shaddock, D. M. (2005). Lead-free solder joint reliability – State of the art and perspectives. International Microelectronics and Packaging Society, 2, 72–83.
  • Solozhenkin, P. M. , & Lyubavina, L. (1979). The bacterial leaching of antymony and bismuth bearing ores and the utilization of sewage waters. In Biogeochemistry of ancient and modern environments in conference on biogeochemistry in relation to the mining industry and environmental pollution, Canberra, Australia, 26 Aug–4 Sep, (pp. 615–621). London: Springer.
  • Tomlinson, W. J. , & Collier, I. (1987). The mechanical properties and microstructures of copper and brass joints soldered with eutectic tin-bismuth solder. Journal of Materials Science, 22, 1835–1839. doi: 10.1007/BF01132413.
  • Tsunekawa, M. , Sasaki, Y. , Nakamura, Y. , Ito, M. , Hiroyoshi, N. , & Yoo, K. (2008). Dispersion-flocculation behavior of fine lead particles in an organic solvent. Materials Transactions, 49, 2119–2123. doi: 10.2320/matertrans.M-MRA2008822.
  • Wood, E. P. , & Nimmo, K. L. (1994). In search of new lead-free electronic solders. Journal of Electronic Materials, 23, 709–713. doi: 10.1007/BF02651363.
  • Yoo, K. , Lee, J. , Lee, K. , Kim, B. , Kim, M. , Kim, S. , & Pandey, B. D. (2012). Recovery of Sn, Ag and Cu from waste Pb-free solder using nitric acid leaching. Materials Transactions, 53, 2175–2180.
  • Zhang, B. , Li, Q. , Shen, W. , & Min, X. (2012). Recovery of bismuth and antimony metals from pressure-leaching slag. Rare Metals, 31, 102–106. doi: 10.1007/s12598-012-0471-1.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.