328
Views
0
CrossRef citations to date
0
Altmetric
Original Article

Durability against wood-destroying fungi of sweet chestnut and mixed sweet chestnut-poplar OSB

, , &
Pages 851-857 | Received 06 Jul 2023, Accepted 22 Nov 2023, Published online: 18 Dec 2023

References

  • Adua, M., 2000. The chestnut culture in Italy towards 2000. Ecologia Mediterranea, 26, 15–31. doi:10.3406/ecmed.2000.1888.
  • Aires, A., Carvalho, R., and Saavedra, M.J., 2016. Valorization of solid wastes from chestnut industry processing: Extraction and optimization of polyphenols, tannins and ellagitannins and its potential for adhesives, cosmetic and pharmaceutical industry. Waste Management, 48, 457–464. doi:10.1016/j.wasman.2015.11.019.
  • Amusant, N., et al., 2009. Biological properties of an OSB eco-product manufactured from a mixture of durable and non-durable species and natural resins. European Journal of Wood and Wood Products, 67, 439–447. doi:10.1007/s00107-009-0335-z.
  • BM TRADA, 2023. TimberWISE 4.1 (2023/24), pp. 700. TRADA Bookshop (UK). https://bookshop.trada.co.uk/bookshop/view/fccd3211-37b8-4ec9-b9c7-7fdb2f13b473.
  • Broda, M., 2020. Natural compounds for wood protection against fungi – A review. Molecules, 25 (15), 3538. doi:10.3390/molecules25153538.
  • Cai, L., et al., 2020. β-Cyclodextrin-allyl isothiocyanate complex as a natural preservative for strand-based wood composites. Composites Part B: Engineering, 196, 108037. doi:10.1016/j.compositesb.2020.108037.
  • Campo, M., Pinelli, P., and Romani, A., 2016. Hydrolyzable tannins from sweet chestnut fractions obtained by a sustainable and eco-friendly industrial process. Natural Product Communications, 11 (3), 409–415.
  • Cetera, P., et al., 2018. Physico-mechanical properties of thermo-treated poplar OSB. Forests, 9 (6), 345. doi:10.3390/f9060345.
  • Chavenetidou, M., Kakavas, K.V., and Birbilis, D., 2020. Shrinkage and swelling of Greek chestnut wood (Castanea sativa Mill.) in relation to extractive presence. Iop Conference Series: Materials Science and Engineering, Volume 908, 5th international Conference on Energy Materials and Applications. 6-9 May 2020, Paris (France). doi:10.1088/1757-899X/908/1/012004.
  • Conedera, M., Tinner, W., Krebs, P., de Rigo, D., and Caudullo, G., 2016. Castanea sativa in Europe: distribution, habitat, usage and threats. In J. San-Miguel-Ayanz, D. de Rigo, G. Caudullo, T. Houston Durrant and A. Mauri, eds., European Atlas of Forest Tree Species. Luxembourg: Publ. Off. EU, 78–79.
  • Das, A.K., et al., 2020. Review on tannins: Extraction processes, applications and possibilities. South African Journal of Botany, 135, 58–70. doi:10.1016/j.sajb.2020.08.008.
  • De Windt, I., et al., 2013. Statistical analysis of durability tests - Part 1: Principles of distribution fitting and application on laboratory tests. The International Research Group on Wood Protection, 44th annual meeting, 16-20/06/2013, Stockholm, Sweden, Doc IRG/WP 13-20504, p. 12.
  • Eichhorn, S., et al., 2017. Determination of the phenolic extractive content in sweet chestnut (Castanea sativa Mill.) Wood. Wood Research, 62, 181–196. http://www.woodresearch.sk/cms/determination-of-the-phenolic-extractive-content-in-sweet-chestnut-castanea-sativa-mill-wood/.
  • EN113-3:2023, Durability of Wood and Wood-Based Products. Test Method Against Wood Destroying Basidiomycetes. Part 3: Assessment of Durability of Wood-Based Panels. Brussels, Belgium: European Committee for Standardization.
  • EN 1995-1-1:2005, Eurocode 5: Design of Timber Structures - Part 1-1: General - Common Rules and Rules for Buildings. Brussels, Belgium: European Committee for Standardization.
  • En 300:2006, Oriented Strand Boards (OSB) - Definitions, Classification and Specifications. Brussels, Belgium: European Committee for Standardization.
  • EN 326-1:1994, Wood-based Panels - Sampling, Cutting and Inspection - Part 1: Sampling and Cutting of Test Pieces and Expression of Test Results. Brussels, Belgium: European Committee for Standardization.
  • EN 335:2013, Durability of Wood and Wood-Based Products – Use Classes: Definitions, Application to Solid Wood and Wood-Based Products. Brussels, Belgium: European Committee for Standardization.
  • EN 350:2016, Durability of Wood and Wood-Based Products – Testing and Classification of the Durability to Biological Agents of Wood and Wood-Based Materials. Brussels, Belgium: European Committee for Standardization.
  • EPF, 2023. Annual report 2020–2021 oriented strand board. European Panel Federation, Brussels. Available online: https://europanels.org/ [accessed on 02 Oct 2023].
  • Faraji, F., 2005. Study on the natural durability of mixed plywood panels composed the durable and non-durable veneers. Life Sciences [q-bio]. ENGREF (AgroParisTech), 2005. English. ffNNT: ff. ffpastel-00001664, pp. 247, https://pastel.archives-ouvertes.fr/pastel-00001664.
  • Gagić, T., Knez, Ž,, and Škerget, M., 2019. Hydrothermal hydrolysis of sweet chestnut (Castanea sativa) tannins. Journal of the Serbian Chemical Society, 84, 1–14. doi:10.2298/JSC190711108G.
  • Gérard, J., et al., 2011. Tropix 7 (Version 7.5.1) [Computer software]. CIRAD. doi:10.18167/74726F706978.
  • Militz, H., Busetto, D., and Hapla, F., 2003. Investigation on fungal durability and sorption properties of Italian Chestnut (Castanea sativa Mill.) from coppice stands. Holz als Roh- und Werkstoff, 61, 133–141. doi:10.1007/s00107-002-0357-2.
  • Okino, E.Y.A., Teixeira, D.E., and Del Menezzi, C.H.S., 2007. Post-thermal treatment of oriented strandboard (OSB) made from cypress (Cupressus glauca Lam.). Maderas. Ciencia y Tecnología, 9 (3), 199–210. doi:10.4067/S0718-221X2007000300001.
  • Papadopoulos, A., 2021. Fungal durability of acetylated OSB in ground stake test: total decay after 102 months of testing. January 2011. European Journal of Wood and Wood Products, 70, 1–3. doi:10.1007/s00107-011-0547-x.
  • Schultz, T.P., and Nicholas, D.D., 2002. Development of environmentally-benign wood preservatives based on the combination of organic biocides with antioxidants and metal chelators. Phytochemistry, 61 (5), 555–560. doi:10.1016/S0031-9422(02)00267-4.
  • Sen, S., et al., 2017. Larvicidal activities of some bark and wood extracts against wood-damaging insects. Maderas. Ciencia y Tecnología, 19 (3), 273–284. doi:10.4067/S0718-221X2017005000023.
  • Spavento, E., et al., 2019. Susceptibility of Populus x euramericana ‘I-214’ of Spanish origin to xylophagous attacks: durability tests for its possible inclusion in European standard. Forest Systems, 28 (2), e008. doi:10.5424/fs/2019282-14660.
  • Tabacchi, G., et al., 2007. INFC – Le Stime Di Superficie 2005–Prima Parte. Inventario Nazionale Delle Foreste E Dei Serbatoi Di Carbonio (in Italian). MiPAF–Corpo Forestale dello Stato-Ispettorato Generale-CRA–ISAFA: Trento, Italy, 2007; p. 409.
  • Theomen, H., Irle, M., and Sernek, M., 2010. Wood Based Panels. An Introduction for Specialists. London, UK: Brunel University Press, 283.
  • Tomak, E.D., and Gonultas, O., 2018. The wood preservative potentials of Valonia, Chestnut, Tara and Sulphited oak tannins. Journal of Wood Chemistry and Technology, 38 (3), 183–197. doi:10.1080/02773813.2017.1418379.
  • Van Acker, J., et al., 2003. Biological durability of wood in relation to end-use. Holz als Roh- und Werkstoff, 61, 35–45. doi:10.1007/s00107-002-0351-8.
  • Van Acker, J., Stevens, M., and De Clercq, E., 2001. Evaluation of the European standard ENV 12038 for durability testing of plywood. The International Research Group on Wood Protection, 32nd annual meeting, 20-25/05/2001, Nara, Japan, Doc IRG/WP 01-20237, p. 13.
  • Van Acker, J., Van den Bulcke, J., Forsthuber, B., and Grüll, G. 2023. Wood preservation and wood finishing. In P. Niemz, A. Teischinger, and D. Sandberg, eds. Springer Handbook of Wood Science and Technology. Cham: Springer Handbooks. Springer.793–872.
  • Van den Bulcke, J., et al., 2011. Moisture dynamics and fungal susceptibility of plywood. International Biodeterioration and Biodegradation, 65 (5), 708–716. doi:10.1016/j.ibiod.2010.12.015.
  • Yurkewich, J.I., Castaño, C., and Colinas, C., 2017. Chestnut red stain: Identification of the fungi associated with the costly discolouration of Castanea sativa. Forest Pathology, 47, e12335. doi:10.1111/efp.12335.
  • Zanuttini, R., et al., 2020a. Thermo-vacuum treatment of Poplar (Populus spp.) plywood. Holzforschung, 74 (1), 60–67. doi:10.1515/hf-2019-0049.
  • Zanuttini, R., et al., 2020b. Preliminary assessment of sweet chestnut and mixed sweet chestnut-poplar OSB. Forests, 11, 496. doi:10.3390/f11050496.
  • Zanuttini, R., Negro, F., and Cremonini, C., 2021. Hardness and contact angle of thermo-treated poplar plywood for biobuilding. iForest - Biogeosciences and Forestry, 14, 274–277. doi:10.3832/ifor3662-014.