Microstructure and permeability of concrete with glass powder addition conserved in the sulphatic environment

, , &
Pages 219-237 | Received 05 Jan 2014, Accepted 24 Jun 2014, Published online: 30 Jul 2014

References

  • Abbas, M., Carcassès, M., & Ollivier, J.-P. (2000). The importance of gas permeability as addition to the compressive strength of concrete. Magazine of Concrete Research, 52, 1–6.10.1680/macr.2000.52.1.1
  • ACI 116R-90. (2000, March 16). Cement and concrete terminology, technical documents, American concrete institute.
  • Alonso, C., Andrade, C., Castellote, M., & Castro, P. (2000). Chloride threshold values to depassivate reinforcing bars embedded in a standardized OPC mortar. Cement and Concrete Research, 30, 1047–1055.10.1016/S0008-8846(00)00265-9
  • Behim, M., & Boucetta, A. (2009). Effet des additions micronisées sur l’écoulement des bétons autoplaçant (laitier de haut fourneau, filler calcaire et Poudre de verre). T. 2. Performance of materials, SBEIDCO, Algérie, October 12–14, 423–430.
  • Bentalha, M. (2007). Influence de l’introduction de fibres métalliques sur le comportement différé d’une matrice cimentaire. Caractérisation - Comportement monotone – Microstructure ( Thèse doctorat d’état). Université Mentouri, Constantine, Algeria.
  • Chaïd, R., Jauberthie, R., Boukhaled, A., & Talah, A. (2009). Endommagement, déformations et microstructure des BHP de pouzzolane. T. 2. Performance of materials, First International Conference on Sustainable Built Environement Infrastructures in Developing Countries, ENSET – Oran, October 12–14, 2009, 117–124.
  • Carsana, M., Frassoni, M., & Bertolini, L. (2014). Comparison of ground waste glass with other supplementary cementitious materials. Cement and Concrete Composites, 45, 39–45.10.1016/j.cemconcomp.2013.09.005
  • Corinaldesi, V., Gnappi, G., Moriconi, G., & Montenero, A. (2004). Reuse of ground waste glass as aggregate for mortars. Waste Management, 25, 197–201.
  • De Castro, S., & de Brito, J. (2013). Evaluation of the durability of concrete made with crushed glass aggregates. Journal of Cleaner Production, 41, 7–14.
  • Du, H., & Tan, K.-H. (2013). Use of waste glass as sand in mortar: Part II – Alkali–silica reaction and mitigation methods. Cement and Concrete Composites, 35, 118–126.10.1016/j.cemconcomp.2012.08.029
  • Idir, R., Cyr, M., & Tagnit-Hamou, A. (2010). Use of fine glass as ASR inhibitor in glass aggregate mortars. Construction and Building Materials, 24, 1309–1312.10.1016/j.conbuildmat.2009.12.030
  • Kojima, T., Takagi, N., & Haruta, K. (2000). Expanding characteristics of mortar in glass powder produced from waste bottles, 673–682. 11th International Conference on Alkali Aggregate Reaction. Quebec, Canada, June 2000, 673–1282.
  • Lea, S. (2004). Chemistry of cement and concrete, fourth Edition by Peter C. Hewlett. pp. 241–289. San Diego: Elsevier Science & Technology Books.
  • Lee, G., Ling, T.-C., Wong, Y.-L., & Poon, C.-S. (2011). Effects of crushed glass cullet sizes, casting methods and pozzolanic materials on ASR of concrete blocks. Construction and Building Materials, 25, 2611–2618.10.1016/j.conbuildmat.2010.12.008
  • Matos, A.-M., & Sousa-Coutinho, J. (2012). Durability of mortar using waste glass powder as cement replacement. Construction and Building Materials, 36, 205–215.10.1016/j.conbuildmat.2012.04.027
  • Moesgaarda, M., Herfort, D., Steenberg, M., Kirkegaard, L.-F., & Yue, Y. (2011). Physical performances of blended cements containing calcium aluminosilicate glass powder and limestone. Cement and Concrete Research, 41, 359–364.10.1016/j.cemconres.2010.12.005
  • Nonnet, E., Lequeux, N., & Boch, P. (1999). Elastic properties of high alumina cement castables from room temperature to 1600°C. Journal of the European Ceramic Society, 19, 1575–1583.10.1016/S0955-2219(98)00255-6
  • Oliveira, R., de Brito, J., & Veiga, R. (2013). Incorporation of fine glass aggregates in renderings. Construction and Building Materials, 44, 329–341.10.1016/j.conbuildmat.2013.03.042
  • Penacho, P., de Brito, J., & Veiga, R.-M. (2014). Physico-mechanical and performance characterization of mortars incorporating fine glass waste aggregate. Cement and Concrete Composites, 50, 47–59.10.1016/j.cemconcomp.2014.02.007
  • Platret, G. (2002). Suivi de l’hydratation du ciment et de l’évolution des phases solides dans les bétons par analyse thermique, caractéristiques microstructurales et propriétés relatives à la durabilité des bétons. Méthodes de mesure et d’essai de laboratoire, In Méthode d’essai n° 58, Laboratoire Central des Ponts et Chaussées, 2002.
  • Roz-Ud-Din, N., & Parviz, S. (2012). Strength and durability of recycled aggregate concrete containing milled glass as partial replacement for cement. Construction and Building Materials, 29, 368–377.
  • Scherer, K.-R. (1995). Cross-cultural patterns. In D. Levinson, J. Ponzetti, & P. Jorgenson (Eds.), Encyclopedia of human emotions (Vol. 1, pp. 147–156). New York, NY: Macmillan.
  • Schwarz, N., Cam, H., & Neithalath, N. (2008). Influence of a fine glass powder on the durability characteristics of concrete and its comparison to fly ash. Cement and Concrete Composites, 30, 486–496.10.1016/j.cemconcomp.2008.02.001
  • Schwarz, N., & Neithalath, N. (2008). Influence of a fine glass powder on cement hydration: comparison to fly ash and modelling the degree of hydration. Cement and Concrete Research, 38, 429–436.10.1016/j.cemconres.2007.12.001
  • Serpa, D., Santos Silva, A., de Brito, J., Pontes, J., & Soares, D. (2013). ASR of mortars containing glass. Construction and Building Materials, 47, 489–495.
  • Shayan, A., & Xu, A. (2005). Performance of glass powder as a pozzolanic material in concrete: A field trial on concrete slabs. Cement and Concrete Research, 36, 457–468.
  • Shi, C., Wu, Y., Riefler, C., & Wang, H. (2005). Characteristics and pozzolanic reactivity of glass powder. Cement and Concrete Research, 35, 987–993.10.1016/j.cemconres.2004.05.015
  • Tagnit, A., & Nkinamubanzib, P.-C. (2001). Les ajouts cimentaires et le développement durable, journée d’étude technique, 19 septembre 2001, Note trimestrielle d’information du Centre d’Etudes et de Services Technologiques de l’Industrie des Matériaux de Construction, CETIM, Algérie.
  • Taha, B., & Nounu, G. (2007). Using lithium nitrate and pozzolanic glass powder in concrete as ASR suppressors. Cement and Concrete Composites, 30, 497–505.
  • Wang, H., & Huang, W. (2010). Durability of self-consolidating concrete using waste LCD glass. Construction and Building Materials, 24, 1008–1013.10.1016/j.conbuildmat.2009.11.018
  • Yammine, J. (2007). Rhéologie des bétons fluides à hautes performances : relations entre formulations, propriétés rhéologiques, physico-chimie et propriétés mécaniques. Thèse de Doctorat de l’Ecole Normale Supérieure de Cachan, ENSC, France.
  • Zeroub, H. (2012). Valorisation du verre dans l’élaboration de béton durable (Approche expérimentale). Magister en sciences et génie des matériaux (Option : Physico-chimie des matériaux minéraux), Algérie, 2012.
  • Zuber, B., & Marchand, J. (2004). Predicting the volume instability of hydrated cement systems upon freezing using poro-mechanics and local phase equilibria. Materials and Structures, 37, 257–270.10.1617/14165

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.