Comparison of biaxial and uniaxial longitudinal rupture tests for determination of residual creep life of ferritic heat-exchanger tubing

Pages 442-446 | Published online: 02 Dec 2013

References

  • R. V. HART: Met. Technol., 1976,3, 1.
  • E. L. ROBINSON: Trans. ASME, 1938, 60,777.
  • D. A. WOODFORD: Paper presented at the internat. conf. on 'Creep and fatigue', Sheffield, 1–5 April 1974, Institution of Mechanical Engineers.
  • A. CHITTY, and D. DUVAL: Paper presented at the joint internat. conf. on ‘Creep’, London, 1963, Institution of Mechanical Engin-eers.
  • Project 2021 Report, 1976, Electrical Research Association.
  • R. B. CARRUTHERS and R. V. DAY: Report No. SSD/NE/R138; Central Electricity Generating Board.
  • Report No. ISO/TC 17SC 10/EPT-SG (Secretariat 46) MG/ OF/417/72; 1972, London, International Standards Organisa-tion.
  • British Standard 1500, Pt 1; 1969, London, British Standards Institution.
  • R. V. HART: Met. Technol., this issue, p.447.
  • A. B. WILDER et al J. Met., 1954, 6, 764.
  • H. R. VOORHEES: ‘Literature survey on creep damage in metals’, STP 391, 60; 1965, Philadelphia, American Society of Testing and Materials.
  • M.J. COLLINS: personal communication, 1976.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.