- Peng J, Wang S, Liu L and Dong Y: ‘A study on dephosphorization of hot metal pretreatment by low fluoride slag’, Special Steel, 2009, 30, (1), 54–57.
- Wang S, Dong Y, Zhou Y and Peng J: ‘Study on low fluoride dephosphorization slag of hot metal’, J. Chin. Rare Earth Soc., 2010, 28, 500–504.
- Mizukami H, Ishikawa M and Hirata T: ‘Dissolution mechanism of fluorine in aqueous solution from fluorine containing synthetic slag’, ISIJ Int., 2004, 44, (3), 623–629.
- Wang H, Zhang Y, Guo S, Chen E and Dong Y: ‘Effect of oxygen potential on De–Si and De–P during hot metal pretreatment’, J. Iron. Steel Res., 2000, 12, (6), 11–15.
- Huang X: ‘Principles of steel metallurgy’; 2002, Beijing, Metallurgical Industry Press.
- Tian Z, Kong X, Cai K, Wang X, Wang T, Shi H and Zhu L: ‘Deep dephosphorization ability of BaO–CaO–CaF2 flux for liquid steel’, J. Univ. Sci. Technol. Beijing, 2005, 27, (3), 294–297.