References
- Sawaragi Y., Ogawa K., Kato S. and Natori A.: ‘Development of the economical 18-8 stainless steel (0·1C–18Cr–9Ni–3Cu–Nb–N) having high elevated temperature strength for fossil fired boilers’, Sumitomo Search, 1992, 48, 50–58.
- Sawaragi Y.: ‘The development of a new 18-8 austenitic stainless steel (0·1C–18Cr–9Ni–3Cu–Nb–N) with high elevated temperature strength for fossil fired boilers’, Mech. Behav. Mater., 1991, 4, 589–594.
- Sawaragi Y., Otsuka N., Senba H. and Yamamoto S.: ‘Properties of a new 18-8 austenitic steel tube for fossil fired boilers after service exposure with high elevated temperature strength’, Sumitomo Search, 1994, 56, 34–43.
- Igarashi M.: ‘Creep properties of heat resistant steels and super alloys’; 2004, Heidelberg, Springer-Verlag.
- Peng K. P., Qian K. W. and Chen W. Z.: ‘Effect of dynamic strain aging on high temperature properties of austenitic stainless steel’, Mater. Sci. Eng. A, 2004, A379, 372–377.
- Sklenicka V. and Kucharova K.: ‘Long-term creep behavior of 9–12% Cr power plants’, Mater. Charact., 2003, 51, 35–48.
- Iseda A., Okada H., Semba H. and Igarashi M.: ‘Long term creep properties and microstructure of Super304H, TP347HFG and HR3C for a-USC boilers’, Energy Mater., 2007, 2, (4), 199–206.
- Peng B. C., Zhang H. X. and Hong J.: ‘Effect of aging on the impact toughness of 25Cr–20Ni–Nb–N steel’, Mater. Sci. Eng. A, 2010, A527, 1957–1961.
- Saito N. and Komai N.: 2007 Proc. ASME Pressure Vessels and Piping Conf.–Proc. 8th Int. Conf. on ‘Creep and fatigue at elevated temperatures–CREEP’, TX: San Antonio, USA, 2007.7, Pressure Vessels & Piping Div, ASME, 211–216.
- ‘Petroleum and natural gas industries. Calculation of heater-tube thickness in petroleum refineries’, 6th edn, API STD 530:2008, BSI Standards, London, UK.
- ‘Metallic materials – tensile testing at ambient temperature’, 2nd edn, ISO 6982:1998, ISO, Geneva, Switzerland.
- ‘Metallic materials – Charpy pendulum impact test. Part 1. Test method’, ISO, Geneva, Switzerland, ISO 148-1:2006.
- Chi C. Y., Yu H. Y. and Dong Q. X.: ‘The precipitation strengthening behavior of Cu-rich phase in Nb contained advanced Fe–Cr–Ni type austenitic heat resistant steel for USC power plant application’, Prog. Nat. Sci., 2012, 22, 175–185.
- Fang Y. Y., Zhao J. and Li N. X.: ‘Precipitates in HR3C steel aged at high temperature’, Acta Metall. Sinica, 2010, 46, 844–849.
- Shima J. H., Kozeschnik E., Jung W. S., Lee S. C., Kim D. I. and Suh J. Y.: ‘Numerical simulation of long-term precipitate evolution in austenitic heat-resistant steels’, Calphad, 2010, 34, 105–112.
- Bi H. Y., Wang Z. J., Shimada M. and Kokama H.: ‘Electron microscopic observation of grain boundary in thermomechanical-processed SUS 304 stainless steel’, Mater. Lett., 2003, 57, 2803–2806.
- Hong H. U., Rho B. S. and Nam S. W.: ‘Correlation of the M23C6 precipitation morphology with grain boundary characteristics in austenitic stainless steel’, Mater. Sci. Eng. A, 2001, A318, 285–292.
- Wang J. D. and Gan D.: ‘Effects of grain boundary carbides on the mechanical properties of Inconel 600’, Mater. Chem. Phys., 2001, 70, 124–128.
- Yong Q. L.: ‘The second phase of steel materials’; 2006, Beijing, Metallurgy Industry Press.
- Wagner C.: ‘Potential and current distribution at electrodes with local variations of the polarization parameter’, Electrochim. Acta, 1961, 65, 581–591.
- Lifshitz I. M. and Slyozov V. V.: ‘The kinetics of precipitation from supersaturated solid solutions’, J. Phys. Chem. Solids, 1961, 19, 35–50.