References
- Khameneh AS, Heydarzadeh SM: ‘Effect of grit-blasting parameters on the surface roughness and adhesion strength of sprayed coating’, Surf. Interface Anal., 2010, 42, 551–554.
- Nikolaj G, Bretislav S, Kamil K, Zdenek P: ‘Residual stress depth profile in surface layers of shot-peened decarburised steels’, Proc. Conf. 50th Annual Conf. on ‘Experimental stress analysis’, Tabor, Czech Republic, June 2012, TechSoft Engn; Variel; VUKV; LABTECH; DUO; Zwick Roell; Safibra; HBP Merici Technika; Inova; Air Phoenix; Composite; CompoTech; IMECO TH; Skoda Power; Instron; Derutex; Nikon; NUX, 111–114.
- Scuracchio BG, de Lima NB, Schön CG: ‘Role of residual stresses induced by double peening on fatigue durability of automotive leaf springs’, Mater. Des., 2013, 47, 672–676.
- Yamauchi N, Demizu K, Ueda N, Sone T, Tsujikawa M, Hirose Y: ‘Effect of peening as pretreatment for DLC coatings on magnesium alloy’, Thin Solid Films, 2006, 506, 378–383.
- Toenshoff HK, Karpuschewski B, Mohlfeld A, Seegers H: ‘Influence of stress distribution on adhesion strength of sputtered hard coatings’, Thin Solid Films, 1998, 332, 146–150.
- Bouzakis K.-D, Michailidis N, Hadjiyiannis S, Efstathiou K, Pavlidou E, Erkens G, Rambadt S, Wirth I: ‘Improvement of PVD coated inserts cutting performance, through appropriate mechanical treatments of substrate and coating surface’, Surf. Coat. Technol., 2001, 146, 443–450.
- Klocke F, Schroeder T, Bouzakis E, Klein A: ‘Manipulation of coating and subsurface properties in reconditioning of WC–Co carbide cutting tools’, Surf. Coat. Technol., 2007, 202, 1194–1198.
- Bouzakis K.-D, Skordaris G, Klocke F, Bouzakis E: ‘A FEM-based analytical–experimental method for determining strength properties gradation in coatings after micro-blasting’, Surf. Coat. Technol., 2009, 203, 2946–2953.
- Bouzakis K.-D, Michailidis N, Skordaris G, Bouzakis E, Biermann D, M’Saoubi R: ‘Cutting with coated tools: coating technologies, characterization methods and performance optimization’, Proc. Conf. 62nd General Assembly of CIRP, Hong Kong, China, August 2012, Vol. 61, 703–723.
- Bouzakis K.-D, Bouzakis E, Skordaris G, Makrimallakis S, Tsouknidas A, Katirtzoglou G, Gerardism S: ‘Effect of PVD films wet micro-blasting by various Al2O3 grain sizes on the wear behaviour of coated tools’, Surf. Coat. Technol., 2011, 205, S128–S132.
- Bouzakis K.-D, Klocke F, Skordaris G, Bouzakis E, Gerardis S, Katirtzoglou G, Makrimallakis S: ‘Influence of dry micro-blasting grain quality on wear behaviour of TiAlN coated tools’, Wear, 2011, 271, 783–791.
- Barbatti C, Garcia J, Pitonak R, Pinto H, Kostka A, Di Prinzio A, Staia MH, Pyzalla AR: ‘Influence of micro-blasting on the microstructure and residual stresses of CVD kappa-Al2O3 coatings’, Surf. Coat. Technol., 2009, 203, 3708–3717.
- Gelfi M, Bontempi E, Roberti R, Depero LE: ‘X-ray diffraction Debye Ring Analysis for STress measurement (DRAST): a new method to evaluate residual stresses’, Acta Mater., 2004, 52, 583–589.
- Cullity BD, Stock SR: ‘Elements of X-ray diffraction’, 3rd edn; 2001, Upper Saddle River, NJ, Prentice Hall.
- Oden M, Ericsson C, Hakasson G, Ljungcrantz H: ‘Microstructure and mechanical behaviour of arc-evaporated Cr–N coatings’, Surf. Coat. Technol., 1999, 114, 39–51.
- Sebastiani M, Piccoli M, Bemporad E: ‘Effect of micro-droplets on the local residual stress field in CAE-PVD thin coatings’, Surf. Coat. Technol., 2013, 215, 407–412.
- Attar F, Johannesson T: ‘Adhesion and X-ray elastic constant evaluation of CrN coating’, Thin Solid Films, 258–, 1995.
- Bouzakis KD, Skordaris G, Bouzakis E: ‘Method for determining coating’s strength changes after inducing plastic or elastic residual stresses’, Proc. Eng., 2011, 19, 34–39.
- Gelfi M, La Vecchia GM, Lecis N, Troglio S: ‘Relationship between through-thickness residual stress of CrN-PVD coatings and fatigue nucleation sites’, Surf. Coat. Technol., 2005, 192, 263–268.
- Baragetti S, Gelfi M, La Vecchia GM, Lecis N: ‘Fatigue resistance of CrN thin films deposited by arc evaporation process on H11 tool steel and 2205 duplex stainless steel’, Fatigue Fract. Eng. Mater. Struct., 2005, 28, 615–21.