182
Views
7
CrossRef citations to date
0
Altmetric
Original Article

Coating formation, fracture mode and cavitation performance of Fe40Al deposited by cold gas spraying

, , , &
Pages 853-859 | Received 17 Oct 2014, Accepted 07 Nov 2014, Published online: 21 Nov 2014

References

  • C. T. Liu and J. O. Stiegler: ‘Ordered intermetallics. Properties and selection: nonferrous alloys and special purpose materials’, in ‘Metals handbook’, 10th edn, Vol. 2, ‘Properties and selection: nonferreous alloys and special-purpose materials’, 913–941; 1990, Materials Park, OH, ASM International.
  • S. C. Deevi and V. K. Sikka: ‘Nickel and iron aluminides: an overview on properties, processing and applications’, Intermetallics, 1996, 4, 357–375. doi: 10.1016/0966-9795(95)00056-9
  • N. Cinca and J. M. Guilemany: ‘Thermal spraying of transition metal aluminides: an overview’, Intermetallics, 2012, 24, 60–72. doi: 10.1016/j.intermet.2012.01.020
  • J. M. Guilemany, N. Cinca, J. Fernández and S. Sampath: ‘Erosion, abrasive and friction wear behaviour of iron aluminide coatings sprayed by HVOF’, J. Therm. Spray Technol., 2008, 17, (5–6), 762–773. doi: 10.1007/s11666-008-9252-7
  • B. Xu, Z. Zhu, W. Zhang and S. Ma: ‘The microstructure and high-temperature sliding wear behavior of Fe-Al coating produced by high velocity arc spraying’, Proc. Int. Thermal Spray Conf. on ‘Advances in technology and application’, Osaka, Japan, 2004, ASM International, 1052–1055.
  • B. Xu, Z. Zhu, S. Ma, W. Zhang and W. Liu: ‘Sliding wear behavior of Fe-Al and Fe-Al/WC coatings prepared by high velocity arc spraying’, Wear, 2004, 257, 1089–1095. doi: 10.1016/j.wear.2004.05.012
  • A. Y. Mosbah, D. Wexler and A. Calka: ‘Abrasive wear of WC-FeAl composites’, Wear, 2005, 258, 1337–1341. doi: 10.1016/j.wear.2004.09.061
  • M. Ahmadian, D. Wexler, T. Chandra and A. Calka: ‘Abrasive wear of WC-FeAl-B and WC-Ni3Al-B composites’, Int. J. Refract. Met. Hard Mater., 2005, 23, 155–159. doi: 10.1016/j.ijrmhm.2004.12.002
  • C. Testani, A. Di Gianfrancesco, O. Tassa and D. Pocci: ‘FeAl intermetallics and applications: an overview’, Proc. Int. Symp. on ‘Nickel and iron aluminides: processing, properties and applications’, Cincinnati, OH, 1996, 213–222.
  • R. Jasionowski and Z. Dariusz: ‘The effect of aluminium content on the cavitational erosion resistance of Fe-Al(B2) alloys’, Proc. 15th Int. Conf. on ‘Properties of water and steam’, 2008.
  • C. M. Hansson: ‘Cavitation erosion’, in ’Metals handbook’, 10th edn, Vol. 18, ‘Friction, lubrication, and wear technology’, 315–333; 1990, Materials Park, OH, ASM International.
  • R. Singh, S. K. Tiwari and S. K. Mishra: ‘Cavitation erosion in hydraulic turbine components and mitigation by coatings: current status and future needs’, J. Mater. Eng. Perform., 2012, 21, (7), 1539–1551. doi: 10.1007/s11665-011-0051-9
  • H. T. Wang, C. J. li, G. J. Yang, C. X. Li, Q. Zhang and W. Y. Li: ‘Microstructural characterization of cold-sprayed nanostructured FeAl intermetallic compound coating and its ball-milled feedstock powders’, Proc. Thermal Spray Conf. on ‘Global coating solutions’, Beijing, China, 2007, ASM International, 135–140.
  • H. Wang, C. Li, G. Yang, C. Li, P. Gao and Q. Zhang: ‘Deposition characteristics of Fe/Al composite coating fabricated by cold spraying’, Proc. Thermal Spray Conf. on ‘Crossing borders’, Maastricht, The Netherlands, 2008, ASM International, 123–129.
  • H.-T Wang, C.-J Li, G.-J Yang and C.-X Li: ‘Cold spraying of Fe/Al powder mixture: coating characteristics and influence of heat treatment on the phase structure’, Appl. Surf. Sci., 2008, 255, 2538–2544. doi: 10.1016/j.apsusc.2008.07.127
  • T. Sugama: ‘Y2O3-sealed Ni-Al protective coatings for Inconel’, Surf. Coat. Technol., 1998, 106, (2–3), 106–116. doi: 10.1016/S0257-8972(98)00502-7
  • Q. Zhang, C. Li, X. Wang, Z. Ren, C. Li and G. Yang: ‘Formation of NiAl intermetallic compound by cold spraying of ball-milled Ni/Al alloy powder through postannealing treatment’, J. Therm. Spray Technol., 2008, 17, (5–6), 715–720. doi: 10.1007/s11666-008-9225-x
  • T. Novoselova, S. Celotto, R. Morgan, P. Fox and W. O’Neill: ‘Formation of TiAl intermetallics by heat treatment of cold-sprayed precursor deposits’, J Alloys Compd, 2007, 436, 69–77. doi: 10.1016/j.jallcom.2006.06.101
  • N. Cinca, A. List, F. Gärtner, J. Fernández, J. M. Guilemany and T. Klassen: ‘Deformation and adherence of Fe40Al- particles in cold gas spraying’, Proc. Int. Thermal Spray Conf., Busan, Korea, 2013, ASM International, 207–301.
  • N. Cinca, A. List, F. Gärtner, J. M. Guilemany and T. Klassen: ‘Influence of spraying parameters on cold gas spraying of iron aluminide intermetallics’, Proc. Les Rencontres Internationales sur la Projection Thermique (6RIPT), European Thermal Spray Association (ETSA), Proceedings RIPT 2013, CD Edition, Limoges.
  • J. Bystrzycki: ‘Static recrystallization of shock-wave (explosively) deformed Fe±40 at% Al±Zr±B intermetallic’, Intermetallics, 2000, 8, 89–98. doi: 10.1016/S0966-9795(99)00071-0
  • H. Assadi, F. Gärtner, T. Stoltenhoff and H. Kreye: ‘Bonding mechanism in cold gas spraying’, Acta Mater., 2003, 51, 4379–4394. doi: 10.1016/S1359-6454(03)00274-X
  • T. Schmidt, , F. Gärtner, H. Assadi and H. Kreye: ‘Development of a generalized parameter window for cold spray deposition’, Acta Mater., 2006, 54, 729–742. doi: 10.1016/j.actamat.2005.10.005
  • T. Stoltenhoff, H. Kreye and H. J. Richter: ‘An analysis of the cold spray process and its coatings’, J. Therm. Spray Technol., 2002, 11, (4), 542–550. doi: 10.1361/105996302770348682
  • I. Baker and D. J. Gaydosh: ‘Flow and fracture of Fe-Al’, Mater. Sci. Eng., 1987, 96, 147–158. doi: 10.1016/0025-5416(87)90549-0
  • M. A. Crimp and K. M. Vedula: ’ Effect of boron on the tensile properties of B2 FeAl ’, Mater. Sci. Eng., 1986, 78, 193–200. doi: 10.1016/0025-5416(86)90323-X
  • H. Xiao and I. Baker: ‘The temperature dependence of the flow and fracture of Fe-40Al’, Scr. Metall. Mater., 1993, 28, 1411–1416. doi: 10.1016/0956-716X(93)90491-A
  • R. L. Fleischer: ‘Intermetallic compounds for strong high-temperature materials: status and potential’, Annu. Rev. Mater. Sci., 1989, 19, 231–263. doi: 10.1146/annurev.ms.19.080189.001311
  • I. Baker, H. Xiao, O. Klein, C. Nelson and J. D. Whittenberger: ‘The effect of temperature and Fe:Al ratio on the flow and fracture of FeAl’, Acta Metal. Mater., 1995, 43, (4), 1723–1730. doi: 10.1016/0956-7151(94)00369-S
  • Y. Yang, I. Baker, G. T. Gray and C. Cady: ‘The yield stress anomaly in stoichiometric FeAl at high strain rate’, Scr. Mater., 1999, 40, (4), 403–408. doi: 10.1016/S1359-6462(98)00448-5
  • C. F. Naude and A. T. Ellis: ‘On the mechanism of cavitation damage by non-hemispherical cavities collapsing in contact with a solid boundary’, J. Basic Eng., 1961, 83, 648–656. doi: 10.1115/1.3662286
  • R. Canavelis: ‘Jet impact and cavitation damage’, J. Basic Eng., 1968, 3, 355–367. doi: 10.1115/1.3605106
  • R. H. Richman and W. P. McNaughton: ‘Correlation of cavitation erosion behavior with mechanical properties of metals’, Wear, 1990, 140, (1), 63–82. doi: 10.1016/0043-1648(90)90122-Q

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.