Surface properties of tannin treated wood during natural and artificial weathering

, , &
Pages 150-157 | Received 20 Dec 2012, Accepted 31 May 2013, Published online: 18 Nov 2013

References

  • Arndt U. 2006. Untreated timber in external situations. Detail 46: 1136–1140.
  • Bächle H, Zimmer B, Windeisen E, Wegener G. 2010. Evaluation of thermally modified beech and spruce wood and their properties by FT-NIR spectroscopy. Wood Sci. Technol. 44: 421–433.
  • Barton FE, Himmelsbach DS, Duckworth JH, Smith MJ. 1992. Two-dimensional vibration spectroscopy: correlation of mid- and near-infrared region. Appl. Spectrosc. 46: 420–429.
  • Bernardis AC, Popoff O. 2009. Durability of Pinus Elliottii wood impregnated with quebracho Colorado (Schinopsis Balansae) bio-protectives extracts and CCA. Maderas 11(2): 107–115.
  • Broman NO. 2000. Means to measure the aesthetic properties of wood. PhD thesis. Lulea University of Technology, Lulea, Sweden.
  • Colom X, Carrillo F, Nogués F, Garriga P. 2003. Structural analysis of photodegraded wood by means of FTIR spectroscopy. Polym. Degrad. Stabil. 80: 543–549
  • EN 113. 1997. European standard. Wood preservatives. Test method for determining the protective effectiveness against wood destroying basidiomycetes. Determination of the toxic values.
  • EN 927-6. 2006. European standard. Paints and varnishes – coating materials and coating systems for exterior wood. Part 6: Exposure of wood coatings to artificial weathering using fluorescent UV and water.
  • Evans PD, Michell AJ, Schmalzl KJ. 1992. Studies of the degradation and protection of wood surfaces. Wood Sci. Technol. 26: 151–163.
  • Evans PD, Owen NL, Schmid S, Webster RD. 2002. Weathering and photostability of benzoylated wood. Polym. Degrad. Stabil. 76: 291–303.
  • Evans PD, Urban K, Chowdhury MJA. 2008. Surface checking of wood is increased by photodegradation caused by ultraviolet and visible light. Wood Sci. Technol. 42: 251–265.
  • Evans PD, Gibson SK, Cullis I, Liu C, Sebe G. 2013. Photostabilization of wood using low molecular weight phenol formaldehyde resin and hindered amine light stabilizer. Polym. Degrad. Stabil. 98: 158–168.
  • Faix O, Böttcher JH. 1992. The influence of particle size and concentration in transmission and diffuse reflectance spectroscopy of wood. Holz Roh Werkst. 50: 221–226.
  • Faix O, Németh K. 1988. Monitoring of wood photodegradation by DRIFT-spectroscopy. Holz Roh Werkst. 46: 112.
  • Feist WC, Hon DNS. 1984. Chemistry of weathering protection. In Rowell 1984, 401–574.
  • George B, Suttie E, Merlin A, Deglise X. 2005. Photodegration and photostabilisation of wood – the state of the art. Polym. Degrad. Stabil. 88: 268–274
  • Grüll G, Scheiger I, Forsthuber B. 2006. Greywood – Technisches Verfahren zur Vergrauung von Holzoberflächen für den Außenbereich. In Haller 2006, 1–15.
  • Hagerman AE. 1988. Extraction of tannin from fresh and preserved leaves. J. Chem. Ecol. 14(2): 453–461.
  • Hon DNS. 2001. Weathering and photochemistry of wood. In Hon and Shiraishi 2001, 513–546.
  • Hon DNS, Chang S-T. 1984. Surface degradation of wood by ultraviolet light. J. Polym. Sci. Polym. Chem. Ed. 22: 2227–2241.
  • Hon DNS, Feist WC. 1981. Free radical formation in wood: the role of water. Wood Sci. 14(1):41–48.
  • Huang X, Kocaefe D, Boluk Y, Boluk Y, Kocaefe Y, Pichette A. 2012. Effect of surface preparation on the wettability of heat-treated jack pine wood surface by different liquids. Eur. J. Wood Prod. 70: 711–717.
  • Jebrane M, Sèbe G, Cullis I, Evans PD. 2009. Photostabilization of wood using aromatic vinyl esters. Polym. Degrad. Stabil. 94(2): 151–157.
  • Laks PE, McKaig PA, Hemingway RW. 1988. Flavonoid biocides: wood preservatives based on condensed tannins. Holzforschung 42(5): 299–306.
  • Lewis J. 1995 Preservation of wood with phenol formaldehyde resorcinol resins. US Patent 5.461.108.
  • Kalnins MA, Feist WC. 1993. Increase in wettability of wood with weathering. Forest Prod. J. 43(2): 55–57.
  • Kishino M, Nakano T. 2004. Artificial weathering of tropical woods. Part 1: Changes in wettability. Holzforschung 58: 552–557.
  • Kuo M.-L, Hu N. 1991. Ultrastructural changes of photodegradation of wood surfaces exposed to UV. Holzforschung 45: 347–353.
  • Kučera LJ, Sell J. 1987. Die Verwitterung von Buchenholz im Holzstrahlbereich. Holz Roh Werkst. 45: 89–93.
  • Michell AJ. 1993. FTIR spectroscopic studies of the reactions of wood and of lignin model compounds with inorganic agents. Wood Sci. Technol. 27: 69–80.
  • Michell AJ, Schimleck LR. 1996. NIR spectroscopy of woods from Eucalyptus globulus. Appita J. 49(1): 23–26.
  • Norrström H. 1969. Light absorbing properties of pulp and pulp components. Part 1. Method. Svensk Papperstidning 72(2): 25–28.
  • Osborne BG, Fearn T, Hidle PH. 1993. Practical NIR spectroscopy with applications in food and beverage analysis. Essex: Pearson Education Limited.
  • Owen NL, Thomas DW. 1989. Infrared studies of ‘hard’ and ‘soft’ woods. Appl. Spectrosc. 43: 451–455.
  • Pizzi A. 1994. Advanced wood adhesive technology. New York: Dekker.
  • Savitzky A, Golay MJE. 1964. Smoothing and differentiation of data by simplified least squares procedures. Anal. Chem. 36: 1627–1639.
  • Schwanninger M, Rodriguez JC, Pereira H, Hinterstoisser B. 2004a. Effects of short-time vibratory ball milling on the shape of FT-IR spectra of wood and cellulose. Vibr. Spec. 36: 23–40.
  • Schwanninger M, Hinterstoisser B, Gradinger C, Messner K, Fackler K. 2004b. Examination of spruce wood biodegraded by Cerioriopsis subvermispora using near and mid infrared spectrosc. J. Near Infrared Spectrosc. 12: 397–409.
  • Sealy-Fisher VJ, Pizzi A. 1992. Increased pine tannins extraction and wood adhesives development by phlobaphenes minimization. Eur. J. Wood Prod. 50(5): 212–220.
  • Sen S, Tascioglu C, Tirk K. 2009. Fixation, leachability, and decay resistance of wood treated with some commercial extracts and wood preservative salts. Int. Biodet. Biodegr. 63(2): 135–141.
  • Singh T, Singh AP. 2012. A review on natural products as wood protectant. Wood Sci. Technol. 46: 851–870.
  • Sudiyani Y, Takahashi M, Imamura Y, Minato K. 1999. Physical and biological properties of chemically modified wood before and after weathering. Wood Res.: Bull. Wood Res. Inst. Kyoto Univ. 86(1): 1–6.
  • Tascioglu C, Yalcin M, De Troya T, Sivrikaya H. 2012. Termiticidal properties of some wood bark extracts used as wood preservatives. Bioresources 7(3): 2960–2969.
  • Thevenon MF, Tondi G, Pizzi A. 2009. High performance tannin resin-boron wood preservatives for outdoor end-uses. Eur. J. Wood Prod. 67: 89–93.
  • Tolvaj L, Faix O. 1995. Artificial ageing of wood monitored by DRIFT spectroscopy and CIE L*a*b* colour measurements. Holzforschung 49: 397–404.
  • Tondi G, Wieland S, Lemenager N, Petutschnigg A, Pizzi A, Thevenon MF. 2012a. Fungal and termites resistance of tannin boron wood preservatives: efficacy of tannin in fixing boron. Bioresources 7(1): 1238–1252.
  • Tondi G, Wieland S, Wimmer T, Thevenon MF, Pizzi A, Petutschnigg A. 2012b. Tannin-boron preservatives for wood buildings: mechanical and fire properties. Eur. J. Wood Prod. 70(5): 689–696.
  • Tondi G, Palanti S, Wieland S, Thevenon MF, Petutschnigg A, Schnabel T. 2012c. Durability of tannin-boron-treated timber. Bioresources 7(4): 5138–5151.
  • Tondi G, Thevenon MF, Mies B, Standfest G, Petutschnigg A, Wieland S. 2013. Impregnation of Scots pine and beech with tannin solutions: effect of viscosity and wood anatomy in wood infiltration. Wood Sci. Technol. 47(3), 615–626.
  • Tsuchikawa S, Siesler HW. 2003. Near-infrared spectroscopic monitoring of the diffusion process of deuterium-labeled molecules in wood. Part I: Softwood. Appl. Spectrosc. 57: 667–674.
  • Windeisen E, Bächle H, Zimmer B, Wegener G. 2009. Relations between chemical changes and mechanical properties of thermally treated wood. Holzforschung 63: 773–778.
  • Zucker WV. 1983. Tannins: does structure determine function? An ecological perspective. Am. Nat. 121(3): 335–363.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.