- Fujikawa, H. and Otsuka, N. Growth Behavior of oxide scale formed on Cr-Mo steels in steam. Nippon Kagaku Kaishi, No. 1, 45-52 (1998). ( in Japanese)
- Fujikawa, H. and Otsuka, N. Effect of Si content on the oxidation behavior of Cr-Mo steels in steam. Nippon Kagaku Kaishi, No. 1, 53-59 (1998). ( in Japanese)
- Griess, J. C., DeVan, J. H. and Maxwell, W. A. Long term corro-sion of Cr-Mo steels in superheated steam at 482 and 538 C. Mate-rials Performance, 21, 18–24 (1982).
- Hurdus, M. H., Tomlinson, L. and Titchmarsh, J. M. Observation of oscillating reaction rates during the isothermal oxidation of terrific steels. Oxidation of Metals, 34 (5/6), 429-464 (1990).
- Ueda, M., Nanko, M., Kawamura, K. and Maruyama, T. Micro-structure development of scales formed in the early stage of steam oxidation of Fe-Cr ferritic alloys at elevated temperatures. Materi-als at High Temperatures, 18 (8), 37-42 (2001).
- Ueda, M., Nanko, M., Kawamura, K. and Maruyama, T. Formation and disappearance of an internal oxidation zone in the initial stage of the steam oxidation of Fe-9Cr-0.265i terrific steel. Materials at High Temperatures, 20 (2), 109-114 (2003).
- Norton, F. J. Gas permeation through the vacuum envelope. Trans. 8th Vacuum Symposium, Pergamon Press, New York, 8-16 (1962).
- Barin, I. Thermochemical Data of Pure Substances, 3rd edn, VCH Verlagsgesellschaft mbH, Weinheim (1995).
- Yamazaki, S. Control of high temperature oxidation of Si steel un-der low oxidation potential. Materia Japan, 37 (3), 179-183 (1998). ( in Japanese)
- Takada, J., Yamamoto, S. Kikuchi, S. and Adachi, M. Internal oxi-dation of Fe—Al alloys in the a-phase region. Oxidation of Metals, 25 (1/2), 93-105 (1986).
- Swisher, J. H. and Turkdogan, E. T. Solubility, permeability, and diffusivity of oxygen in solid iron. Transactions of the Metal-lurgical Society of AIME, 239, 426–431 (1967).