Microscopical investigation of steamside oxide on X20CrMoV121 superheater tubes

, , &
Pages 355-360 | Published online: 24 Oct 2014

REFERENCES

  • Wright, I.G. and Dooley, R.B. (2010) A review of the oxida-tion behaviour of structural alloys in steam. Int. Mater Rev., 55, 129–167.
  • Larsen, O.H., Frandsen, R.B. and Blum, R. (2004) Exfoliation of steamside oxides from austenitic superheaters. Proc. Werkstoffe und Qualitatssicherung 10111 Marz 2004, Dortmund, VGB Powertech.
  • Montgomery, M., Jensen, S.A., Rasmussen, E and Vilhelm-sen, T. (2009) Fireside corrosion and steamside oxidation of 9-12%Cr martensitic steels exposed for long term testing. Corros. Eng. Sci. Techn., 44 (3), 196-210.
  • Hansson, A.N., Montgomery, M. and Somers, M.A.J. (2009) Oxidation of X20 in water vapour: The effect of temperature and oxygen partial pressure. Oxidat. Met., 71, 201–218.
  • Bamba, G., Wouters, Y, Galerie, A., Borchardt, G., Shimada, S., Heintz, O. and Chevalier, S. (2007) Inverse growth trans-port in thermal chromia scales on Fe-15Cr steels in oxygen and in water vapour and its effect on scale adhesion. Scr Mater., 57, 671 —674.
  • Montgomery, M., Hansson, A.N., Vilhelmsen, T. and Jensen, S.A. Mater. Corros., in press.
  • Zurek, J., Wessel, E., Niewolak, L., Schmitz, E, Kern, T.U., Singheiser, L. and Quadakkers, W.J. (2004) Anomalous tem-perature dependence of oxidation kinetics during steam oxida-tion of ferritic steels in the temperature range 550-650 C. Corros. Sci., 46, 2301 — 2317.
  • Hultquist, G., Tveten, B., Hörnlund, E., Limbäck, M. and Haugsrud, R. (2001) Self-repairing Metal oxides. Oxidat. Met., 56, 313–346.
  • Nakai, M., Kensuke, N., Murata, Y, Morinaga, M., Matsuda, S. and Karmo, M. (2005) Correlation of High temperature steam oxidation with hydrogen dissolution in pure iron and ternary high-chromium ferritic steel. ISIJ Int., 45, 1066–1072.
  • Hansson, A.N. and Montgomery, M. (2006) Field Testing of TP347H FG at Ultra Supercritical Steam Conditions. Proceed-ings Materials for Advanced Power Engineering, 1663–1672.
  • Komai, N., Masuyama, E and Igarishi, M. (2005) 10 year experience with T23 (2.25Cr-1.6W) and T122 (12Cr-0.4Mo-2W) in a power boiler. J Press. Vess. Techn., 127, 190-196.

Reprints and Corporate Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

To request a reprint or corporate permissions for this article, please click on the relevant link below:

Academic Permissions

Please note: Selecting permissions does not provide access to the full text of the article, please see our help page How do I view content?

Obtain permissions instantly via Rightslink by clicking on the button below:

If you are unable to obtain permissions via Rightslink, please complete and submit this Permissions form. For more information, please visit our Permissions help page.